The effect of pulsed laser welding on hot cracking susceptible region size and weld pool internal geometry of Inconel 718: Numerical and experimental approaches

2021 ◽  
Vol 35 ◽  
pp. 787-794
Author(s):  
Amin Keivanloo ◽  
Homam Naffakh-Moosavy ◽  
Reza Miresmaeili
Procedia CIRP ◽  
2018 ◽  
Vol 74 ◽  
pp. 679-682
Author(s):  
Fritz Lange ◽  
Antoni Artinov ◽  
Marcel Bachmann ◽  
Michael Rethmeier ◽  
Kai Hilgenberg

2012 ◽  
Vol 20 (3) ◽  
pp. 534-540
Author(s):  
吴东江 WU Dong-jiang ◽  
王占宏 WANG Zhan-hong ◽  
马广义 MA Guang-yi ◽  
杨义彬 YANG Yi-bin ◽  
郭玉泉 GUO Yu-quan ◽  
...  

Author(s):  
DongSheng Zhao ◽  
Liangliang Wu ◽  
TianFei Zhang ◽  
Lele Kong ◽  
YuJun Liu

Hot cracking is a serious problem in welding of Invar alloy. The weld hot cracking susceptibility of Invar was evaluated using pulsed laser welding on fish-bone sheet experiment. The pulse wave consisted of preheating pulse and welding pulse. Hot cracks that formed along the grain boundary propagated from the weld upper surface to the inside. The experiments show that adding a preheating pulse can effectively reduce the hot cracking susceptibility of Invar alloy. Finite Element Modeling (FEM) calculations and experimental measurement results show that the welding temperature gradient and cooling rate decrease with increasing preheating pulse duration. However, as the preheating pulse duration increases, the hot cracking susceptibility of the Invar alloy does not decrease all the time, but decreases first and then increases. This is because the increase of heat input leads to the increase of shrinkage plastic strain when the preheating pulse duration increases. The maximum tensile strength of the butt welded joint of the Invar alloy was 467.3 MPa, which is 92.3% of the base metal when the preheating pulse duration is 3 ms.


2019 ◽  
Vol 35 (4) ◽  
pp. 338-343 ◽  
Author(s):  
DongSheng Zhao ◽  
ZhenYu Huang ◽  
YuJun Liu ◽  
Tangjun Miao

Hot cracking is one of the major challenges in laser welding of Invar alloy. In this study, welding hot cracking susceptibility experiments are conducted with fish-bone‐type Invar alloy sheets under pulsed laser welding condition. The pulse wave consists of two distinct power levels: welding pulse and post-heating pulse. The welding temperature field can be controlled by changing the duration of the post-heating pulse. The results of experimental measurements and finite element method calculation show that increasing of the post-heating pulse duration leads to a decline in the cooling rate of weld metal within the brittle temperature range, although the welding hot cracking susceptibility decreases at first and then increases. Neither the heat input nor the cooling rate is the only decisive factor for hot cracking during the welding process.


2012 ◽  
Vol 44 (5) ◽  
pp. 1521-1528 ◽  
Author(s):  
Jao-Hwa Kuang ◽  
Tsung-Pin Hung ◽  
Chih-Kuan Chen

2021 ◽  
pp. 1-7
Author(s):  
A. V. Bogdanov ◽  
B. V. Buketkin ◽  
A. A. Kholopov ◽  
A. V. Perestoronin ◽  
R. Galiullin

Measurement ◽  
2019 ◽  
Vol 134 ◽  
pp. 25-32 ◽  
Author(s):  
Jie Xu ◽  
Yi Luo ◽  
Liang Zhu ◽  
Jingtao Han ◽  
Chengyang Zhang ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document