Design-oriented stress-strain model for FRP-confined ultra-high performance concrete (UHPC)

2022 ◽  
Vol 318 ◽  
pp. 126200
Author(s):  
JinJing Liao ◽  
Jun-Jie Zeng ◽  
Qi-Ming Gong ◽  
Wai-Meng Quach ◽  
Wan-Yang Gao ◽  
...  
2020 ◽  
Vol 858 ◽  
pp. 182-187
Author(s):  
Yu Dong Han ◽  
Zhen Bo Wang ◽  
Zi Jie Hong ◽  
Jian Ping Zuo ◽  
Chang Liu ◽  
...  

The brittleness and easiness to crack expose marine concrete to serious durability issues. Engineered Cementitious Composites (ECC), as a new generation of ultra high performance concrete, is expected to overcome the strain-softening properties of traditional concrete and realize function of crack-width control. In this paper, the sulfate erosion of ECC under drying-wetting cycles was modelled in laboratory test. And the compression test on cylinders after exposure to different erosion cycles was implemented to obtain the stress-strain properties. The results disclose that sulfate erosion imposes significant influence on both the nonlinear ascending and descending portions of the stress-strain properties of ECC. As the erosion period extended, ECC strength undergoes an obvious increase. And the descending section of the eroded ECC shows a significant stress drop, which is quite different from that before erosion. Additionally, a simple analytical model was proposed to provide satisfactory prediction of the stress-strain properties of ECC exposed to sulfate erosion.


2011 ◽  
Vol 243-249 ◽  
pp. 1145-1155
Author(s):  
Jian Yang ◽  
Zhi Fang ◽  
Gong Lian Dai

Ultra High Performance Concrete (UHPC), which has very special properties that are remarkably different to the properties of normal and high performance concrete, is being increasingly used for the construction of structure. In this paper, an experimental program was formulated to investigate the characteristics of complete stress-strain curve of UHPC in uniaxial compression and flexural behaviors of prestressed UHPC beams. The particular focus was the influence of the partial prestress ratio and jacking stress on the flexural response of UHPC beams. The results show that UHPC is of good deformability, and a general form of the serpentine curve is proposed to represent the complete stress-strain relationship of UHPC in compression. The tests of beams demonstrated that the UHPC beams have an excellent behavior in load carrying capacity, crack distribution and deformability, their ultimate deflection can reach 1/34~1/70 of the span. Based on this investigation, theoretical correlations for the prediction structure response of UHPC beam are proposed.


2021 ◽  
Vol 8 ◽  
Author(s):  
Jinkang Lian ◽  
Chao Hu ◽  
Tengfei Fu ◽  
Yulin Wang

Ultra-high performance concrete (UHPC) has the inherent potential to self-sensing capability due to its inclusion of steel fibers or other electrically conductive materials. Many studies have investigated the electrical and piezoresistive properties of UHPC. With the incorporation of micro steel fibers, carbon nanotubes, carbon nanofibrils, or nano graphite platelets, it opens up great potential to allow UHPC to effectively sense stress, strain, and crack damage. Therefore, the UHPC-based structures can achieve the functionality of structure health monitoring (SHM). This article reviews the recent advances in self-sensing capability of various UHPC-based materials with the focus on sensing capability and mechanisms. Future applications and challenges are also discussed.


PCI Journal ◽  
2020 ◽  
Vol 65 (6) ◽  
pp. 35-61
Author(s):  
Chungwook Sim ◽  
Maher Tadros ◽  
David Gee ◽  
Micheal Asaad

Ultra-high-performance concrete (UHPC) is a special concrete mixture with outstanding mechanical and durability characteristics. It is a mixture of portland cement, supplementary cementitious materials, sand, and high-strength, high-aspect-ratio microfibers. In this paper, the authors propose flexural design guidelines for precast, prestressed concrete members made with concrete mixtures developed by precasters to meet minimum specific characteristics qualifying it to be called PCI-UHPC. Minimum specified cylinder strength is 10 ksi (69 MPa) at prestress release and 18 ksi (124 MPa) at the time the member is placed in service, typically 28 days. Minimum flexural cracking and tensile strengths of 1.5 and 2 ksi (10 and 14 MPa), respectively, according to ASTM C1609 testing specifications are required. In addition, strain-hardening and ductility requirements are specified. Tensile properties are shown to be more important for structural optimization than cylinder strength. Both building and bridge products are considered because the paper is focused on capacity rather than demand. Both service limit state and strength limit state are covered. When the contribution of fibers to capacity should be included and when they may be ignored is shown. It is further shown that the traditional equivalent rectangular stress block in compression can still be used to produce satisfactory results in prestressed concrete members. A spreadsheet workbook is offered online as a design tool. It is valid for multilayers of concrete of different strengths, rows of reinforcing bars of different grades, and prestressing strands. It produces moment-curvature diagrams and flexural capacity at ultimate strain. A fully worked-out example of a 250 ft (76.2 m) span decked I-beam of optimized shape is given.