Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V
1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted
200 ksi (1379 MPa) Tensile Strength Capability