Steel, Corrosion and Heat-Resistant, Bars and Wire, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V, Consumable Electrode Melted, 1800 °F (982 °C) Solution Treated and Work-Strengthened, Capable of 160 ksi (1103 MPa) Tensile Strength