A. Tarancón

The use of cermets as fuel electrodes for solid oxide electrolysis cells requires permanent circulation of reducing gas, e.g. H2 or CO, so called safe gas, in order to avoid oxidation of the metallic phase. Replacing metallic based electrodes by pure oxides is therefore proposed as an advantage for the industrial application of solid oxide electrolyzers. In this work, full-ceramic symmetrical solid oxide electrolysis cells have been investigated for steam/CO2 co-electrolysis. Electrolyte supported cells with La0.75Sr0.25Cr0.5Mn0.5O3−δ reversible electrodes have been fabricated and tested in co-electrolysis mode using different fuel compositions, from pure H2O to pure CO2, at temperatures between 850–900 °C. Electrochemical impedance spectroscopy and galvanostatic measurements have been carried out for the mechanistic understanding of the symmetrical cell performance. The content of H2 and CO in the product gas has been measured by in-line gas micro-chromatography. The effect of employing H2 as a safe gas has also been investigated. Maximum density currents of 750 mA cm−2 and 620 mA cm−2 have been applied at 1.7 V for pure H2O and for H2O : CO2 ratios of 1 : 1, respectively. Remarkable results were obtained for hydrogen-free fuel compositions, which confirmed the interest of using ceramic oxides as a fuel electrode candidate to reduce or completely avoid the use of safe gas in operation minimizing the contribution of the reverse water shift reaction (RWSR) in the process. H2 : CO ratios close to two were obtained for hydrogen-free tests fulfilling the basic requirements for synthetic fuel production. An important increase in the operation voltage was detected under continuous operation leading to a dramatic failure by delaminating of the oxygen electrode.


2019 ◽  
Vol 12 (10) ◽  
pp. 3053-3062 ◽  
Author(s):  
Beom-Kyeong Park ◽  
Qian Zhang ◽  
Peter W. Voorhees ◽  
Scott A. Barnett

The fracture at the electrode/electrolyte interface occurs for a critical oxygen pressure and an associated electrode overpotential.