Excitation of magnetic inhomogeneities in three-layer ferromagnetic structure with different parameters of the magnetic anisotropy and exchange

2015 ◽  
Vol 385 ◽  
pp. 217-221 ◽  
Author(s):  
E.G. Ekomasov ◽  
R.R. Murtazin ◽  
V.N. Nazarov
2015 ◽  
Vol 233-234 ◽  
pp. 51-54 ◽  
Author(s):  
Evgeniy G. Ekomasov ◽  
Azamat M. Gumerov ◽  
Ramil R. Murtazin ◽  
Roman V. Kudryavtsev ◽  
Andrey E. Ekomasov ◽  
...  

The domain walls dynamics and generation and evolution of magnetic inhomogeneities of soliton type, emerging in a thin flat layer with the parameters of the magnetic anisotropy, which are different from other two thick layers of the five-layer ferromagnetic structure, were investigated.


2016 ◽  
Vol 6 (2) ◽  
pp. 138-140 ◽  
Author(s):  
E. G. Ekomasov ◽  
A. M. Gumerov ◽  
R. V. Kudryavtsev

2016 ◽  
Vol 845 ◽  
pp. 195-198 ◽  
Author(s):  
Evgeniy Ekomasov ◽  
Ramil Murtazin ◽  
Oksana Bogomazova ◽  
Vladimir Nazarov

The dynamics of domain walls (DW) in three-layered ferromagnetic was studied. The minimum velocity required for a DW to pass through the spatial modulation region was calculated. The excitation of DW internal oscillation modes and localized magnetic inhomogeneity of breather type was analyzed.


Author(s):  
A.E.M. De Veirman ◽  
F.J.G. Hakkens ◽  
W.M.J. Coene ◽  
F.J.A. den Broeder

There is currently great interest in magnetic multilayer (ML) thin films (see e.g.), because they display some interesting magnetic properties. Co/Pd and Co/Au ML systems exhibit perpendicular magnetic anisotropy below certain Co layer thicknesses, which makes them candidates for applications in the field of magneto-optical recording. It has been found that the magnetic anisotropy of a particular system strongly depends on the preparation method (vapour deposition, sputtering, ion beam sputtering) as well as on the substrate, underlayer and deposition temperature. In order to get a better understanding of the correlation between microstructure and properties a thorough cross-sectional transmission electron microscopy (XTEM) study of vapour deposited Co/Pd and Co/Au (111) MLs was undertaken (for more detailed results see ref.).The Co/Pd films (with fixed Pd thickness of 2.2 nm) were deposited on mica substrates at substrate temperatures Ts of 20°C and 200°C, after prior deposition of a 100 nm Pd underlayer at 450°C.