Germanium-Modified Cordierite Ceramics with Low Thermal Expansion

1986 ◽  
Vol 69 (12) ◽  
pp. 847-851 ◽  
Author(s):  
D. K. AGRAWAL ◽  
V. S. STUBICAN ◽  
Y. MEHROTRA
2018 ◽  
Vol 281 ◽  
pp. 99-104
Author(s):  
Meng Li Qin ◽  
Xi Tang Wang ◽  
Zhou Fu Wang ◽  
Yan Ma ◽  
Hao Liu

In order to synthesize cordierite ceramics with low thermal expansion coefficient and good properties, in our work, the cordierite ceramics were prepared by using talc, natural containing zirconium kyanite, common kyanite and industrial Al2O3 as raw materials, introducing the right amount of WO3 (introducing tungsten acid) as catalyst. The effects of the introduced WO3 on the phase composition, sintering characters, microstructure and thermal expansion coefficient of the cordierite ceramics were investigated. The results show that the introduction of WO3 can eliminate the intermediate phase magnesia-alumina spinel and promote the formation of cordierite; the as-prepared cordierite ceramics synthesized by using natural containing zirconium kyanite as raw materials have high densification degree and low thermal expansion coefficient (1.53×10-6/°C, Rt~1000 °C).


2010 ◽  
Vol 105-106 ◽  
pp. 802-804 ◽  
Author(s):  
Kai Zhu ◽  
Dao Yuan Yang ◽  
Juan Wu ◽  
Rui Zhang

Cordierite is an excellent material with good thermal shock resistance and used at high temperature for its low thermal expansion coefficient. Cordierite ceramics were prepared by using talc, alumina and kaolin clay as starting materials. The thermal expansion coefficient, phase composition and microstructure were studied and the results showed that: in order to get samples with low thermal expansion coefficient, the optimum chemical composition was a little rich in Al2O3 compared with the theoretical composition, the optimum sintering temperature was 1350°C, and adding 10% starch as pore-forming agent could effectively decreased the thermal expansion coefficient of the samples even to 0.8×10-6/°C. The samples contained majority of cordierite phase, with trace mullite and glass, the acicular cordierite crystals in samples developed very well and there were 10% starch powder used as pore-forming agent in formula. All these were the reasons to decrease the thermal expansion coefficient of cordierite material.


ChemInform ◽  
1987 ◽  
Vol 18 (13) ◽  
Author(s):  
D. K. AGRAWAL ◽  
V. S. STUBICAN ◽  
Y. MEHROTRA

2015 ◽  
Vol 25 (7) ◽  
pp. 330-335 ◽  
Author(s):  
Dong-Min Kim ◽  
◽  
Sook-In Jung ◽  
Hun-Chul Lee ◽  
Sang-Jin Lee

2001 ◽  
Vol 79 (1) ◽  
pp. 6-10 ◽  
Author(s):  
Chong S. Yoon ◽  
Jae H. Kim ◽  
Chang K. Kim ◽  
K.S. Hong

Sign in / Sign up

Export Citation Format

Share Document