Thermoplastic vulcanizates based on epoxidized natural rubber/polypropylene blends: Effect of epoxide levels in ENR molecules

2006 ◽  
Vol 101 (5) ◽  
pp. 3046-3052 ◽  
Author(s):  
Charoen Nakason ◽  
Puripong Wannavilai ◽  
Azizon Kaesaman
2013 ◽  
Vol 844 ◽  
pp. 109-112 ◽  
Author(s):  
Chesidi Hayichelaeh ◽  
Charoen Nakason ◽  
Anoma Thitithammawong

Epoxidized natural rubber (ENR)/Polypropylene (PP) thermoplastic vulcanizates were prepared by melt mixing method in an internal mixer. Influences of different mixing methods for incorporation of processing oil into the TPVs on tensile and dynamic mechanical properties of the TPVs and crystallinity of the PP were investigated. Results show that distribution of processing oil in the ENR/PP TPV is important due to the processing oil can promote and in the same time can interrupt an improvement in elastomeric properties of the TPV. Incorporation of processing oil into the ENR phase by preparation of oil extended ENR (the mixing method 1) before mixing with the PP was the better way to produce the TPV. It promoted the TPV with superior tensile and dynamic mechanical properties than the TPVs prepared from the mixing method 2 and 3 in which the processing oil was directly added into the PP phase. Furthermore, the TPV from the mixing method 1 had less effect of processing oil on the PP crystallization.


2012 ◽  
Vol 602-604 ◽  
pp. 690-695
Author(s):  
Hua Dong Wang ◽  
Rui Wang ◽  
Mao Fang Huang ◽  
Qi Yang

Thermoplastic vulcanizates (TPVs) based on epoxidized natural rubber (ENR) and polypropylene (PP) were prepared in an internal mixer at 180°C. The effects of curing systems (i.e., sulfur and peroxide) on morphological, rheological, thermal and mechanical properties were studied. It is found that the sulfur cured TPVs show higher tensile strength, tear strength and elongation at break than those cured with the DCP systems. The rheological analysis indicates that TPVs cured with DCP system show lower apparent shear viscosity than those with sulfur system. SEM studies show that TPVs vulcanized with DCP system exhibit smaller and finely dispersed rubber domains, which provides it higher thermal stability than sulfur cured TPVs.