Investigation of tungsten concentrate used for alloying in ladle refining process

1994 ◽  
Vol 65 (3) ◽  
pp. 85-89
Author(s):  
Weiqing Chen ◽  
Rongzhang Zhou ◽  
Wan-Wook Huh ◽  
Chang-Hee Rhee
2011 ◽  
Vol 295-297 ◽  
pp. 2647-2650 ◽  
Author(s):  
Hong Ming Wang ◽  
Ting Wang Zhang ◽  
Hua Zhu ◽  
Yong Qi Yan ◽  
Yi Nan Zhao

To avoid slag sticking onto the snorkel during CAS-OB ladle refining process, B2O3-CaO(mass ratio equals 1:1) and CaF2-CaO(mass ratio equals 1:1) were respectively employed as modifiers added to decrease the viscosity of ladle slag. The rotary cylinder method was adopted in the viscosity measurements. The results showed that the modifiers could decrease the viscosity of ladle refining slag remarkably. At 1500°C, the viscosity of ladle slag without any modifiers is about 6.0 Pa·s. But by adding more than 10mass% CaO-B2O3 or CaO-CaF2, the slag viscosity at 1500°C could be decreased lower than 1.0 Pa·s. The mechanism of modifiers decreasing the slag viscosity was analyzed.


1989 ◽  
Vol 29 (2) ◽  
pp. 148-153 ◽  
Author(s):  
Kanehiro Ogawa ◽  
Toshio Onoue

2004 ◽  
Vol 44 (3) ◽  
pp. 636-638 ◽  
Author(s):  
Manabu Iguchi ◽  
Ken-ichiro Miyamoto ◽  
Shintaro Yamashita ◽  
Daisuke Iguchi ◽  
Masafumi Zeze

1999 ◽  
Vol 85 (5) ◽  
pp. 368-374 ◽  
Author(s):  
Katsuhiro FUCHIGAMI ◽  
Masamitsu WAKOH ◽  
Naochika IMAMURA ◽  
Koichi ENDOH ◽  
Akito KIYOSE ◽  
...  

Sign in / Sign up