Recovery of high purity copper from waste printed circuit boards of mobile phones by slurry electrolysis with ammonia-ammonium system

Author(s):  
Jiqin Wang ◽  
Shuyuan Chen ◽  
Xiangfei Zeng ◽  
Jinfeng Huang ◽  
Qian Liang ◽  
...  
10.30544/427 ◽  
2019 ◽  
Vol 25 (2) ◽  
pp. 171-182
Author(s):  
Martina Laubertova ◽  
Marcela Malindzakova ◽  
Jarmila Trpcevska ◽  
Natasa Gajic

Waste printed circuit boards (WPCBs) from discarded mobile phones and smartphones are considerably heterogeneous materials with a high gold content (approx. 490 grams per ton). The aim of our chemical analysis of samples of WPCBs was to determine the amounts of gold using open acid digestion and atomic absorption spectrometry (HR CS AAS). The test samples designated for chemical analysis must genuinely represent the bulk WPCBs from which they are taken. This study aimed to develop a correct sampling procedure to analyze the heterogeneous materials from printed circuit boards; explicitly concerning the influence of particle size on the precision of chemical analysis of WPCBs from discarded mobile phones. Chemical analysis of the representative sample of WPCBs with a grain size fraction of d ≤ 200 μm determined that the gold content was 475 g∙t-1 with a low variation coefficient and low dispersion which indicates very high accuracy of the designed sampling procedure.


2014 ◽  
Vol 13 (10) ◽  
pp. 2601-2607 ◽  
Author(s):  
Jae-chun Lee ◽  
Manoj Kumar ◽  
Min-Seuk Kim ◽  
Jinki Jeong ◽  
Kyoungkeun Yoo

JOM ◽  
2020 ◽  
Author(s):  
Joona Rajahalme ◽  
Siiri Perämäki ◽  
Roshan Budhathoki ◽  
Ari Väisänen

AbstractThis study presents an optimized leaching and electrowinning process for the recovery of copper from waste printed circuit boards including studies of chemical consumption and recirculation of leachate. Optimization of leaching was performed using response surface methodology in diluted sulfuric acid and hydrogen peroxide media. Optimum leaching conditions for copper were found by using 3.6 mol L−1 sulfuric acid, 6 vol.% hydrogen peroxide, pulp density of 75 g L−1 with 186 min leaching time at 20°C resulting in complete leaching of copper followed by over 92% recovery and purity of 99.9% in the electrowinning. Study of chemical consumption showed total decomposition of hydrogen peroxide during leaching, while changes in sulfuric acid concentration were minor. During recirculation of the leachate with up to 5 cycles, copper recovery and product purity remained at high levels while acid consumption was reduced by 60%.