Precision measurement of the pion mass differencemπ−−mπ0

1991 ◽  
Vol 43 (1) ◽  
pp. 46-58 ◽  
Author(s):  
J. F. Crawford ◽  
M. Daum ◽  
R. Frosch ◽  
B. Jost ◽  
P. -R. Kettle ◽  
...  
Author(s):  
G. L. Borchert ◽  
B. Manil ◽  
D. Anagnostopoulos ◽  
J. P. Egger ◽  
D. Gotta ◽  
...  

Author(s):  
Manfred Daum ◽  
Peter-R. Kettle

The most precise value for the pion mass was determined from a precision measurement at PSI of the muon momentum in pion decay at rest, \pi^+ \rightarrow \mu^+ + \nu_{\mu}π+→μ++νμ. The result is m_{\pi^+} = 139.570\,21(14)mπ+=139.57021(14)~MeV/c^22. This value is more precise, however, in agreement with the recent compilation of the Particle Data Group for m_{\pi^-}mπ−. The agreement of m_{\pi^+}mπ+ with the recent measurement. This yields a new quantitative measure of CPT invariance in the pion sector: (m_{\pi^+} - m_{\pi^-})/m_{\pi}(\mbox{av}) = (-2.9 \pm 2.0)\cdot 10^{-6}(mπ+−mπ−)/mπ(av)=(−2.9±2.0)⋅10−6, an improvement by two orders of magnitude.


1991 ◽  
Vol 1 (12) ◽  
pp. 1669-1673 ◽  
Author(s):  
Hans Gerd Evertz ◽  
Martin Hasenbusch ◽  
Mihail Marcu ◽  
Klaus Pinn ◽  
Sorin Solomon

Alloy Digest ◽  
1984 ◽  
Vol 33 (1) ◽  

Abstract INDALLOY 160-190 is a bismth-base low-melting alloy that melts through th temperature range 160-190 F. It shrinks immediately upon solidification, grows back to zero in about one hour and then shows additional growth. This shrinkage-growth behavior makes it an ideal alloy for proof casting and precision measurement of internal dimensions. This alloy originally was developed for use by children for casting soldiers and other small objects. It performs best among the low-melting alloys for spraying in the spray forming of masks and molds and in metallizing. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, and joining. Filing Code: Bi-34. Producer or source: Indium Corporation of America.


2020 ◽  
Vol 28 (11) ◽  
pp. 2429-2436
Author(s):  
Peng XU ◽  
◽  
Yuan-shan LIU ◽  
Jian-guo ZHANG ◽  
◽  
...  

1958 ◽  
Vol 28 (12) ◽  
pp. 809-816
Author(s):  
F. J. BEUTLER ◽  
L. L. RAUCH

Sign in / Sign up

Export Citation Format

Share Document