ELECTROMECHANICAL CHARACTERIZATION OF LANTHANUM-DOPED SODIUM BISMUTH TITANATE CERAMICS

2006 ◽  
Vol 20 (09) ◽  
pp. 475-480 ◽  
Author(s):  
M. APARNA ◽  
M. RAGHAVENDER ◽  
G. PRASAD ◽  
G. S. KUMAR

The effect of lanthanum doping on the electromechanical properties of lanthanum-doped sodium bismuth titanate was studied. The ferroelectric system under investigation was Na 1/2( La x Bi 1-x)1/2 TiO 3 ceramics, with x=0, 0.1, 0.15 and 0.2. Admittance measurements were carried out in the frequency range of 100 Hz to 13 MHz and in the temperature range from room temperature to 550°C. Combined impedance and admittance spectroscopy was used to analyze admittance data. The electromechanical parameters were calculated from the resonant and anti-resonant frequencies obtained from vector admittance plots. The electromechanical coefficients for pure sodium bismuth titanate ceramic samples were found to be much larger than the reported values. Also, it was observed that lanthanum-doping decreased the values of electromechanical coupling coefficients.

2015 ◽  
Vol 27 (1) ◽  
pp. 407-413 ◽  
Author(s):  
D. E. Jain Ruth ◽  
S. M. Abdul Kader ◽  
M. Muneeswaran ◽  
N. V. Giridharan ◽  
D. Pathinettam Padiyan ◽  
...  

2018 ◽  
Vol 54 (7) ◽  
pp. 744-748 ◽  
Author(s):  
E. D. Politova ◽  
A. V. Mosunov ◽  
D. A. Strebkov ◽  
N. V. Golubko ◽  
G. M. Kaleva ◽  
...  

2010 ◽  
Vol 123-125 ◽  
pp. 121-124 ◽  
Author(s):  
Xin Cheng ◽  
Shuang Shuang Liao ◽  
Shi Feng Huang ◽  
Li Li Guo

Sulphoaluminate cement and Lead Niobium-Magnesium Zirconate Titanate ceramic [P(MN)]ZT were used as matrix and functional phase respectively to fabricate 1-3-2 cement-based piezoelectric composites by dice and filling technique. The influences of base thickness on piezoelectric properties, electromechanical properties and acoustic impedance properties of the composites were discussed. The results show that as the base thickness increases, the piezoelectric stain factor d33 increases gradually, while the piezoelectric voltage factor g33 decreases. The planar electromechanical coupling coefficient Kp exhibits the trend of decrease, while the thickness electromechanical coupling coefficient Kt and acoustic impedance show the increasing trend. The mechanical quality factor Qm reaches the minimum (1.49) when base thickness is 2.00 mm. The results reveal that the 1-3-2 piezoelectric composite will be suitable for application by changing the base thickness.


2012 ◽  
Vol 120 (1398) ◽  
pp. 58-63 ◽  
Author(s):  
Warapong KRENGVIRAT ◽  
Srimala SREEKANTAN ◽  
Ahmad-Fauzi b. MOHD NOOR ◽  
Atsunori MATSUDA ◽  
Charoen CHINWANITCHAROEN

2019 ◽  
Vol 45 (10) ◽  
pp. 13269-13274 ◽  
Author(s):  
Ruike Shi ◽  
Yongping Pu ◽  
Jingwei Li ◽  
Xu Guo ◽  
Wen Wang ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document