Effect of Liquid Sodium on Welded AISI Type-304 Stainless-Steel Pipe
Nuclear Applications
◽
10.13182/nt68-a26379
◽
1968
◽
Vol 4
(3)
◽
pp. 154-158
◽
Cited By ~ 3
Author(s):
G. A. Ratz
◽
K. G. Brickner
Keyword(s):
Stainless Steel
◽
Steel Pipe
◽
304 Stainless Steel
◽
Liquid Sodium
◽
Aisi Type
◽
Stainless Steel Pipe
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
Related Documents
Cited By
References
Effect of Long-Time Exposure to Liquid Sodium on a Welded AISI Type 304 Stainless-Steel Pipe
Nuclear Technology
◽
10.13182/nt73-a31242
◽
1973
◽
Vol 17
(2)
◽
pp. 153-159
◽
Cited By ~ 1
Author(s):
G. A. Ratz
Keyword(s):
Stainless Steel
◽
Steel Pipe
◽
304 Stainless Steel
◽
Liquid Sodium
◽
Time Exposure
◽
Aisi Type
◽
Stainless Steel Pipe
◽
Long Time
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
Low temperature sensitization of type 304 stainless steel pipe weld heat affected zone
Metallurgical Transactions A
◽
10.1007/bf02646660
◽
1987
◽
Vol 18
(8)
◽
pp. 1483-1493
◽
Cited By ~ 12
Author(s):
Charles G. Schmidt
◽
Robert D. Caligiuri
◽
Lawrence E. Eiselstein
◽
Sharon S. Wing
◽
Daniel Cubicciotti
Keyword(s):
Stainless Steel
◽
Low Temperature
◽
Heat Affected Zone
◽
Steel Pipe
◽
304 Stainless Steel
◽
Stainless Steel Pipe
◽
Type 304
◽
Type 304 Stainless Steel
◽
Weld Heat
Download Full-text
Correlation of Sensitization with Thermomechanical History of Type 304 Stainless Steel Pipe Joint
MiCon 78: Optimization of Processing, Properties, and Service Performance Through Microstructural Control
◽
10.1520/stp36876s
◽
2009
◽
pp. 306-306-15
Author(s):
YG Nakagawa
◽
T Kawamoto
◽
M Fukagawa
◽
Y Saiga
Keyword(s):
Stainless Steel
◽
Steel Pipe
◽
304 Stainless Steel
◽
Stainless Steel Pipe
◽
History Of
◽
Type 304
◽
Type 304 Stainless Steel
◽
Pipe Joint
Download Full-text
Closeout of IE Bulletin 79-03: Longitudinal weld defects in ASME SA-312 Type 304 stainless steel pipe spools manufactured by Youngstown Welding and Engineering Co
10.2172/6344615
◽
1989
◽
Author(s):
W. J. Foley
◽
R. S. Dean
◽
A. Hennick
Keyword(s):
Stainless Steel
◽
Steel Pipe
◽
304 Stainless Steel
◽
Weld Defects
◽
Stainless Steel Pipe
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
Closeout of IE Bulletin 79-03A: Longitudinal weld defects in ASME SA-312 Type 304 stainless steel pipe
10.2172/6344603
◽
1989
◽
Author(s):
W. J. Foley
◽
R. S. Dean
◽
A. Hennick
Keyword(s):
Stainless Steel
◽
Steel Pipe
◽
304 Stainless Steel
◽
Weld Defects
◽
Stainless Steel Pipe
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
Stress-Corrosion Cracking of a Type 304 Stainless Steel Pipe Caused by Residual Welding Stresses
ASM Failure Analysis Case Histories: Power Generating Equipment
◽
10.31399/asm.fach.power.c0091528
◽
2019
◽
Keyword(s):
Stainless Steel
◽
Stress Corrosion
◽
Stress Corrosion Cracking
◽
Corrosion Cracking
◽
Steel Pipe
◽
304 Stainless Steel
◽
Residual Welding
◽
Stainless Steel Pipe
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
Investigation of Ductile Fracture Properties of Welded Type 304 Stainless Steel Pipe and Large Plan Compact Specimens
Fracture Mechanics: Eighteenth Symposium
◽
10.1520/stp23238s
◽
2009
◽
pp. 134-134-17
◽
Cited By ~ 1
Author(s):
RA Hays
◽
MG Vassilaros
◽
JP Gudas
Keyword(s):
Stainless Steel
◽
Ductile Fracture
◽
Steel Pipe
◽
304 Stainless Steel
◽
Fracture Properties
◽
Stainless Steel Pipe
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
Correlation of acoustic emission with stress intensity factor and plastic zone size for notched tensile specimens of AISI type 304 stainless steel
Materials Science and Technology
◽
10.1179/026708302225006089
◽
2002
◽
Vol 18
(10)
◽
pp. 1133-1141
◽
Cited By ~ 5
Author(s):
C. K. Mukhopadhyay
◽
T. Jayakumar
◽
B. Raj
◽
K. K. Ray
Keyword(s):
Stress Intensity Factor
◽
Stainless Steel
◽
Acoustic Emission
◽
Stress Intensity
◽
Plastic Zone Size
◽
304 Stainless Steel
◽
Zone Size
◽
Aisi Type
◽
Type 304
◽
Type 304 Stainless Steel
Download Full-text
The morphology of oxide film growth on AISI type 304 stainless steel in high temperature water at 300° and 350° C
Journal of Nuclear Materials
◽
10.1016/0022-3115(66)90016-x
◽
1966
◽
Vol 20
(1)
◽
pp. 1-10
◽
Cited By ~ 17
Author(s):
J.M. Francis
◽
W.H. Whitlow
Keyword(s):
Stainless Steel
◽
High Temperature
◽
Oxide Film
◽
Film Growth
◽
304 Stainless Steel
◽
High Temperature Water
◽
Aisi Type
◽
Type 304
◽
Type 304 Stainless Steel
◽
Temperature Water
Download Full-text
Technique for Studying the Kinetics of Intergranular Crack Nucleation on AISI Type 304 Stainless Steel in Oxygenated Water at 289 C
CORROSION
◽
10.5006/0010-9312-25.9.359
◽
1969
◽
Vol 25
(9)
◽
pp. 359-365
◽
Cited By ~ 9
Author(s):
B. E. WILDE
Keyword(s):
Stainless Steel
◽
Intergranular Crack
◽
Crack Nucleation
◽
304 Stainless Steel
◽
Aisi Type
◽
Oxygenated Water
◽
Type 304
◽
Type 304 Stainless Steel
◽
Kinetics Of
Download Full-text
Sign in / Sign up
Close
Export Citation Format
Close
Share Document
Close