Synthesis of Li+ Memorized Spinel Li3Mn0.75O3 by a Solid State Reaction Crystallization Method

2012 ◽  
Vol 178-181 ◽  
pp. 475-478
Author(s):  
Jin He Jiang

The ion-exchanger Li3Mn0.75O3 of spinel type was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 8.3mmol/g for Li+.

2012 ◽  
Vol 549 ◽  
pp. 118-121
Author(s):  
Jin He Jiang

A spinel-type metal compound [LiMn0.5Ti0.75O3], was prepared by a solid state reaction crystallization method. The Li+ extraction/insertion with this material were investigated by X-ray and Kd measurement. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 4.2mmol/g for Li+.


2012 ◽  
Vol 424-425 ◽  
pp. 789-792
Author(s):  
Heng Li

Compound [LiZnPO4], a spinel-type metal compound, was prepared by a solid state reaction crystallization method. The experimental results showed that the Li+extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 4.1 mmol/g for Li+.


2012 ◽  
Vol 457-458 ◽  
pp. 206-209
Author(s):  
Heng Li

Compound [Li1.4Zn0.8PO4], a spinel-type metal compound, was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 6.2 mmol/g for Li+.


2012 ◽  
Vol 554-556 ◽  
pp. 874-877
Author(s):  
Jin He Jiang

Compound [Li2Mn0.5Ti0.5O3], a spinel-type metal compound, was prepared by a solid state reaction crystallization method. The Li+ extraction/insertion with this material were investigated by X-ray and Kd measurement. The chemical analysis showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 7.7mmol/g for Li+.


2012 ◽  
Vol 528 ◽  
pp. 126-129
Author(s):  
Jin He Jiang

Spinel-type metal compound [LiMnTi0.25O3], was prepared by a solid state reaction crystallization method. LiMnTi0.25O3 can be used to separate Li+ in the aqueous solution. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 4.0mmol/g for Li+


2013 ◽  
Vol 842 ◽  
pp. 259-262
Author(s):  
Jin He Jiang ◽  
Wei Yu Dai

Compound [Li0.5Mn1.375O3] was a spinel-type metal compound and was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The characterization results showed that the exchange capacity of Li+ was 2.8mmol/g for Li+. Li0.5Mn1.375O3 is an ion-memory inorganic ion exchanger of Li+. It had a memorial ion-sieve property for Li+.


2012 ◽  
Vol 549 ◽  
pp. 466-469 ◽  
Author(s):  
Jin He Jiang

LiMn0.25TiO3was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of in 0.1mol /L HNO3 solution is 4.3mmol/g for Li+. It had a memorial ion-sieve property for Li+.


2012 ◽  
Vol 549 ◽  
pp. 78-81
Author(s):  
Jin He Jiang

Spinel-type etal oxides, Lithium -manganese oxide Li4Mn0.5O3 was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 12.7mmol/g for Li+.


2012 ◽  
Vol 457-458 ◽  
pp. 26-29
Author(s):  
Heng Li

Lithium-titanium oxide(Li2.5Ti1.375O4) was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 8.1mmol/g for Li+.


2012 ◽  
Vol 554-556 ◽  
pp. 856-859
Author(s):  
Jin He Jiang

Inorganic ion exchanger Li2Mn0.75Ti0.25O3 is synthesized. It was prepared by a solid state reaction crystallization method. The results showed that the Li+ extraction/insertion be progressed mainly by an ion-exchange mechanism. The acid treated samples had an ion exchange capacity of 7.4 mmol•g-1 for Li+. It had a memorial ion-sieve property for Li+.