Synthesis and Lithium Ion Conductivity of MP2O7-Based Solid Electrolytes
2008 ◽
Vol 388
◽
pp. 53-56
◽
Keyword(s):
Phase studies and ac-conductivity measurements were carried out in the compositions M0.8In0.2Li0.2P2O7 [MILP] (M=Sn, Zr, Ti). The bulk conductivities were of the order of ~10-5 Scm-1 at 623 K and higher in the order of TiILP≥ZrILP>SnILP. The activation energies, as expected, became lower in the order of ZrILP<TiILP<SnILP with increasing size of the bottleneck windows for hopping of the Li ions. The order of TiILP≥ZrILP>SnILP in bulk conductivities were not correlated with that of the activation energies probably because of the impureness of the ZrILP sample.