Differential speed rolling (DSR) has been carried out on AZ31 alloys with Mn additions of 0 to 0.6 wt% for investigating the effects of Mn on microstructure, texture, mechanical properties, and formability. The Al–Mn compounds were formed in the sample with a Mn addition of only 0.2 wt% because of its low solid-solubility limit. There were tiny differences among the DSR-processed AZ31 alloys with different Mn contents, while the AZ31 alloy without Mn addition exhibited a more homogeneous microstructure, a weaker basal texture intensity, and a much superior formability together with a larger likelihood of grain growth during annealing. The Mn dissolving in αMg matrix exerted a far stronger influence on the resulting properties compared with those existing in form of the Al–Mn compounds. The Mn solute atoms induced an increase in c/a ratio, which may suppress activity of nonbasal slips and in turn degrade the deformation capability.


2008 ◽  
Vol 488 (1-2) ◽  
pp. 214-220 ◽  
Author(s):  
Xinsheng Huang ◽  
Kazutaka Suzuki ◽  
Akira Watazu ◽  
Ichinori Shigematsu ◽  
Naobumi Saito

Copper ◽  
2007 ◽  
pp. 44-49
Author(s):  
Tetsuo Sakai ◽  
Junya Watanabe ◽  
Naoaki Iwamoto ◽  
Hiroshi Utsunomiya

2007 ◽  
Vol 544-545 ◽  
pp. 395-398 ◽  
Author(s):  
Xin Sheng Huang ◽  
Kazutaka Suzuki ◽  
Akira Watazu ◽  
Ichinori Shigematsu ◽  
Naobumi Saito

An AZ31 (Mg-3Al-1Zn-0.35Mn in mass%) alloy sheet exhibiting the inclination of the basal plane from the rolling plane at about 15º, was fabricated by a DSR processing with a roll speed ratio of 1.167. Compared with the normal rolled sheets, the DSR processed sheets showed a lower 0.2% proof stress, a larger elongation, a smaller r-value and a larger n-value. The Erichsen value at room temperature significantly increased from 2.2 to 3.1, and the deep drawability also improved.


2008 ◽  
Vol 457 (1-2) ◽  
pp. 408-412 ◽  
Author(s):  
Xinsheng Huang ◽  
Kazutaka Suzuki ◽  
Akira Watazu ◽  
Ichinori Shigematsu ◽  
Naobumi Saito

Sign in / Sign up

Export Citation Format

Share Document