Real-time detection of cooling rate using pyrometers in tandem in laser material processing and directed energy deposition

2020 ◽  
Vol 277 ◽  
pp. 128330
Author(s):  
Amal M. Nair ◽  
Gopinath Muvvala ◽  
Sagar Sarkar ◽  
Ashish Kumar Nath
2020 ◽  
Vol 36 ◽  
pp. 101468
Author(s):  
Mohamed A. Naiel ◽  
Deniz Sera Ertay ◽  
Mihaela Vlasea ◽  
Paul Fieguth

2020 ◽  
Vol 1000 ◽  
pp. 375-380
Author(s):  
Desrilia Nursyifaulkhair ◽  
Faris Arief Mawardi ◽  
Nokeun Park ◽  
Eung Ryul Baek ◽  
Sungwook Kim

The alteration in phase morphology of Ti-6Al-4V alloy fabricated using directed energy deposition (DED) was investigated in this study. Owing to the fast cooling rate during DED, the specimen exhibited the diffusionless transformation products of martensite (α′) and massive (αm) phases. In the top layer, the α′ exhibited a needle-like morphology with the width of approximately 0.94 μm. Meanwhile, the αm presented a lamellar structure with α thickness of nearly 0.98 μm. In contrast, the morphology of α′ and αm started to decompose into α+β phase in the bottom layer. Furthermore, the hardness values increased with higher deposition layers. These phenomena could be explained by the effect of repetitive heating, as the nature of DED method during the depositing of new layers. Moreover, it was observed the α thickness of αm in the bottom layer was finer than that in the top layer due to the higher cooling rate.


2008 ◽  
Vol 40 (2) ◽  
pp. 330-336 ◽  
Author(s):  
Jun Xie ◽  
Lide You ◽  
Shuhuai Huang ◽  
Zhengcheng Duan ◽  
Guoqing Chen

Measurement ◽  
2019 ◽  
Vol 135 ◽  
pp. 905-912 ◽  
Author(s):  
Yuan-Jen Chang ◽  
Chih-Yuan Wang ◽  
Jin-Chen Hsu ◽  
Chao-Ching Ho ◽  
Chia-Lung Kuo

Sign in / Sign up

Export Citation Format

Share Document