scholarly journals Formation of Solidification Structure in Twin Roll Casting Process of 18Cr-8Ni Stainless Steel.

1995 ◽  
Vol 35 (6) ◽  
pp. 771-777 ◽  
Author(s):  
Toshiaki Mizoguchi ◽  
Ken-ichi Miyazawa
2013 ◽  
Vol 395-396 ◽  
pp. 209-213
Author(s):  
Zhi Pu Pei ◽  
Hong Yang Zhao ◽  
Xiao Dong Hu ◽  
Dong Ying Ju

Thermal flow finite element simulation was carried out to deeply understand the solidification and deformation phenomena of magnesium alloy in molten zone during twin-roll casting process. The results show that temperature near the nip of the rolls is about 680K based on current conditions, and there are two vortexes in the molten pool during casting, a peak formed at solidus. Due to the metal flows in molten pool and relative rotates of the rolls, temperature field of molten zone is different from normal casting, which will cause the solidification structure changes. An experiment by using a vertical type twin-roll caster was also conducted, and the amount of deformation bands at the joint line is larger than that at the two sides. Substructures can be found due to dynamic recrystallization during casting process.


Metals ◽  
2021 ◽  
Vol 11 (6) ◽  
pp. 952
Author(s):  
Shiju Li ◽  
Bowen Wei ◽  
Wei Yu ◽  
Chen He ◽  
Yong Li ◽  
...  

In this work, a Al-Cu-Li alloy plate with outstanding mechanical properties was successfully prepared with electromagnetic twin-roll casting (TRC) technology. The microstructure of Al-Cu-Li alloy manufactured by conventional mold casting, TRC, and electromagnetic TRC was studied in detail. The action mechanism of electromagnetic oscillation field (EOF) in the TRC process was studied by systematic experimental characterization and numerical simulation. The results show that the EOF will enlarge the circumfluence area in the cast-rolling zone, accelerate the mass transfer and heat transfer in the molten pool, and make the solute field and flow field in the liquid cavity tend to be evenly distributed. Further, the introduction of the EOF will produce the electromagnetic body force F with the maximum strength of 14 N/m3. The F acting on the solidification front will eliminate the accumulation and deposition of Cu2+, Li+, Mg2+, Zn2+, Mn2+ at the dendrite tip and inhibit the growth of dendrites. At the same time, the F can refine the microstructure of the TRC plate, promote the formation of equiaxed crystals, improve the supersaturated solid solubility of solute elements in the a(Al) matrix, and avoid the appearance of obvious solute segregation area or the formation of excessive solute enrichment area. Therefore, the macro-segregation in TRC plate was significantly reduced, the solidification structure was dramatically refined, and the comprehensive properties of the alloy were remarkably improved.


2013 ◽  
Vol 690-693 ◽  
pp. 218-221
Author(s):  
Ting Zhang ◽  
Xiao Ming Zhang ◽  
Zhi Yuan Guo ◽  
Yu Qian Wang ◽  
Cheng Gang Li

Effect of secondary cooling on non-oriented electrical steel strips was investigated. The 2.0 mm thick cast strips contain two compositions were produced by twin-roll casting process, cooled in the air or cooled by spraying water. The microstructure was observed by optical microscopy, and EBSD was used to characterize the texture of the cast strips. The results showed that air-cooling cast strips have uniform and equiaxed grains with average size of 250 μm. The microstructure of the water-spraying cast strips compose of most equiaxed grains and a small number of abnormal big grains. At the same time, the secondary cooling rate mildly affects the cast texture strength but has no influence on the texture type.


2013 ◽  
pp. 989-996 ◽  
Author(s):  
O. Daaland ◽  
A. B. Espedal ◽  
M. L. Nedreberg ◽  
I. Alvestad