The high temperature workability of the ZEK200 Mg-alloy produced by Direct Chill casting (DC) was investigated by torsion testing between 200 and 450°C. The alloy exhibited a higher strength and a slightly lower equivalent strain to fracture than AZ31 and ZM21 produced by DC. The calculation of the constitutive equation gave a value of the activation energy for high temperature deformation close to 175 kJ/mol, in line with those calculated by following the same procedure in AZ31 and ZM21. Partial or complete recrystallization of the deformed structure was observed at 350 and 400°C respectively. Grain growth occurred after recrystallization in the samples tested at 450°C.

2009 ◽  
Vol 57 (9) ◽  
pp. 2812-2822 ◽  
Author(s):  
Eric M. Taleff ◽  
Louis G. Hector ◽  
John R. Bradley ◽  
Ravi Verma ◽  
Paul E. Krajewski

2005 ◽  
Vol 20 (1) ◽  
pp. 13-17 ◽  
Author(s):  
Tiandan Chen ◽  
Martha L. Mecartney

An alumina-based ceramic codispersed with 15 vol% zirconia and 15 vol% mullite (AZM) was synthesized by reactive processing, and the creep behavior was compared to alumina with 30 vol% zirconia (AZ). Constant stress compressive creep behavior for AZM exhibited a stress exponent of 2 and an activation energy of 770 KJ/mol, while a similar stress exponent but lower activation energy of 660 KJ/mol was found for AZ. The strain rate of AZM, however, was more than twice that of the AZ under the same deformation conditions, indicating a better potential for superplastic shape forming.


2013 ◽  
Vol 15 (8) ◽  
pp. 761-766 ◽  
Author(s):  
Chalasani Dharmendra ◽  
Kamineni Pitcheswara Rao ◽  
Yellapregada Venkata Rama Krishna Prasad ◽  
Norbert Hort ◽  
Karl Ulrich Kainer

Sign in / Sign up

Export Citation Format

Share Document