Quantitative Assessment of Submodes of Stress Corrosion Cracking on the Secondary Side of Steam Generator Tubing in Pressurized Water Reactors: Part 3

CORROSION ◽  
2004 ◽  
Vol 60 (2) ◽  
pp. 115-180 ◽  
Author(s):  
R. W. Staehle ◽  
J. A. Gorman
2020 ◽  
Vol 536 ◽  
pp. 152182 ◽  
Author(s):  
Michael R. Ickes ◽  
Joshua McKinley ◽  
Jung-Kun Lee ◽  
Jean M. Smith ◽  
Andrew M. Ruminski ◽  
...  

Author(s):  
L. F. Fredette ◽  
Paul M. Scott ◽  
F. W. Brust

The Mechanical Stress Improvement Process (MSIP) has been used successfully to mitigate intergranular stress corrosion cracking in boiling water reactor (BWR) welded stainless steel piping for many years. The MSIP technique creates compressive residual stresses at the inside surface of the welded joint while producing a slight permanent deformation of the pipe on one side of the weld. A prerequisite for use of MSIP on welded pipes susceptible to primary water stress corrosion cracking (PWSCC) in pressurized water reactors (PWR) is knowledge of the efficacy of the process when applied to dissimilar metal welds common to PWR primary cooling piping. This study uses two and three dimensional finite element models to evaluate the likely residual and operating stress profiles remaining after MSIP for typical dissimilar metal weld configurations, some of which are approved for leak-before-break (LBB) applications in pressurized water reactors.


Author(s):  
G. Angah Miessi ◽  
Peter C. Riccardella ◽  
Peihua Jing

Weld overlays have been used to remedy intergranular stress corrosion cracking (IGSCC) in boiling water reactors (BWRs) since the 1980s. Overlays have also been applied in the last few years in pressurized water reactors (PWRs) where primary water stress corrosion cracking (PWSCC) has developed. The weld overlay provides a structural reinforcement with SCC resistant material and favorable residual stresses at the ID of the overlaid component. Leak-before-break (LBB) had been applied to several piping systems in PWRs prior to recognizing the PWSCC susceptibility of Alloy 82/182 welds. The application of the weld overlay changes the geometric configuration of the component and as such, the original LBB evaluation is updated to reflect the new configuration at the susceptible weld. This paper describes a generic leak-before-break (LBB) analysis program which demonstrates that the application of weld overlays always improves LBB margins, relative to un-overlaid, PWSCC susceptible welds when all the other parameters or variables of the analyses (loads, geometry, operating conditions, analysis method, etc…) are kept equal. Analyses are performed using LBB methodology previously approved by the US NRC for weld overlaid components. The analyses are performed for a range of nozzle sizes (from 6″ to 34″) spanning the nominal pipe sizes to which LBB has been commonly applied, using associated representative loads and operating conditions. The analyses are performed for both overlaid and un-overlaid configurations of the same nozzles, and using both fatigue and PWSCC crack morphologies in the leakage rate calculations and the LBB margins are compared to show the benefit of the weld overlays.