A thermal analysis study on nitriding R6M5 high-speed steel powder

1995 ◽  
Vol 34 (5-6) ◽  
pp. 244-246
Author(s):  
O. A. Mazno ◽  
I. R. Dolgoarshinnykh ◽  
A. A. Yudakov
1988 ◽  
Vol 135 ◽  
pp. 291-297 ◽  
Author(s):  
U. Shuali ◽  
S. Yariv ◽  
M. Steinberg ◽  
M.Muller Vonmoos ◽  
G. Kahr ◽  
...  

1997 ◽  
Vol 253-254 ◽  
pp. 207-209 ◽  
Author(s):  
L.E.A Berlouis ◽  
P.J Hall ◽  
A.J MacKinnon ◽  
A.W Wark ◽  
D Manuelli ◽  
...  

2014 ◽  
Vol 879 ◽  
pp. 169-174
Author(s):  
R. Sauti ◽  
N.A. Wahab ◽  
M.A. Omar ◽  
I.N. Ahmad

This paper reports on the compatibility of waste rubber as binder for M2 High Speed Steel injection moulding. The feedstock was prepared at a powder loading of 65 vol.% using 22μm M2 High Speed Steel powder and the binders consisting of 55wt.% paraffin wax, 21wt.% polyethylene, 14wt.% waste rubber and 10wt.% stearic acid. The specimens were then sintered in vacuum and 95%N2/5%H2 atmosphere. The sintering in vacuum atmosphere occurred within a temperature range from1200°C to 1260°C, whilst the 95%N2/5%H2 atmosphere was carried out within a temperature range from 1220°C to 1300°C. The effects of the sintering atmosphere and temperature on the physical properties, mechanical properties and microstructure were investigated.