Improvement of AISI 304 austenitic stainless steel low-cycle fatigue life by initial and intermittent deep rolling

2018 ◽  
Vol 101 (1-4) ◽  
pp. 435-449 ◽  
Author(s):  
Naoufel Ben Moussa ◽  
Khouloud Gharbi ◽  
Iheb Chaieb ◽  
Nabil Ben Fredj
Author(s):  
Yuichi Fukuta ◽  
Yuichiro Nomura ◽  
Seiji Asada

NUREG/CR-6909 of USA and JSME of Japan proposed new rules for evaluating environmental effects in fatigue analyses of reactors components. These rules were established from a lot of fatigue data with polished specimens under simple loading condition. The effects of surface finish or complex loading condition were reported in some papers, but these data were obtained with the simple shaped specimens. In order to evaluate the effects of surface finish and loading condition and to confirm the applicability of the proposed rules to actual components, Low Cycle Fatigue tests are performed in PWR environment with the specimens cut from 316 austenitic stainless steel welded piping. The pipes are machined to have three levels of surface finish condition and the load pattern simulating the thermal stress is applied to specimens. In this study, the effect of surface finish on fatigue life is included to be small for 316 austenitic stainless steel welded piping. Considering the insensitive region in the current evaluation rule, predicted accuracy is increased and possibility of improving the current rule is indicated.


Author(s):  
Jean Alain Le Duff ◽  
Andre´ Lefranc¸ois ◽  
Jean Philippe Vernot

During mid 2006, ANL issued a NUREG/CR-6909 [2] report that is now applicable in The US for evaluations of PWR environmental effects in the fatigue analysis of new reactor components. In order to assess the conservativeness of the application of this NUREG report, low cycle fatigue (LCF) tests were performed by AREVA NP on austenitic stainless steel specimens in a PWR environment. The selected material exhibits in an air environment a fatigue behavior consistent with the ANL reference “air” mean curve. Tests were performed for two various loading conditions: for fully reverse triangular signal (for comparison purpose with tests performed by other laboratories with same loading conditions) and complex signal, simulating strain variation for actual typical PWR thermal transients. Two surface finish conditions were tested: polished and ground. The paper presents on one side the comparison of environmental penalty factors (Fen = Nair,RT/Nwater) as observed experimentally with the ANL formulation (considering the strain integral method for complex loading), and, on the other hand, the actual fatigue life of the specimen with the fatigue life predicted through the NUREG/CR-6909 application. Low Cycle Fatigue test results obtained on austenitic stainless steel specimens in PWR environment with triangle waveforms at constant low strain rates gives Fen penalty factors close to those estimated using the ANL formulation (NUREG report 6909). On the contrary, it was observed that constant amplitude LCF test results obtained under complex signal reproducing an actual sequence of a cold and hot thermal shock exhibits significantly lower environmental effects when compared to the Fen penalty factor estimated on the basis of the ANL formulations. It appears that the application of the NUREG/CR-6909 [2] in conjunction with the Fen model proposed by ANL for austenitic stainless steel provides excessive margins whereas the current ASME approach seems sufficient to cover significant environmental effect for components.


2015 ◽  
Vol 59 (3) ◽  
pp. 91-98
Author(s):  
V. Šefl

Abstract In this literature review we identify and quantify the parameters influencing the low-cycle fatigue life of materials commonly used in nuclear power plants. The parameters are divided into several groups and individually described. The main groups are material properties, mode of cycling and environment parameters. The groups are further divided by the material type - some parameters influence only certain kind of material, e.g. sulfur content may decreases fatigue life of carbon steel, but is not relevant for austenitic stainless steel; austenitic stainless steel is more sensitive to concentration of dissolved oxygen in the environment compared to the carbon steel. The combination of parameters i.e. conjoint action of several detrimental parameters is discussed. It is also noted that for certain parameters to decrease fatigue life, it is necessary for other parameter to reach certain threshold value. Two different approaches have been suggested in literature to describe this complex problem - the Fen factor and development of new design fatigue curves. The threshold values and examples of commonly used relationships for calculation of fatigue lives are included. This work is valuable because it provides the reader with long-term literature review with focus on real effect of environmental parameters on fatigue life of nuclear power plant materials.


Author(s):  
Hong-Se Son ◽  
Wan-Kyu Choi ◽  
Sung-Choong Woo ◽  
Jong-Cheon Kim ◽  
Jeong-Seok Lee ◽  
...  

Author(s):  
Ikram Abarkan ◽  
Rabee Shamass ◽  
Zineb Achegaf ◽  
Abdellatif Khamlichi

Abstract Mechanical components are frequently subjected to severe cyclic pressure and/or temperature loadings. Therefore, numerical and analytical low cycle fatigue methods become widely used in the field of engineering to estimate the design fatigue lives. The primary aim of this work is to evaluate the accuracy of the most commonly used numerical and analytical low cycle fatigue life methods for specimens made of 316 LN austenitic stainless steel and subjected to fully reversed uniaxial tension-compression loading, in the room temperature condition. It was found that both Maximum shear strain and Brown-Miller criterions result in a very conservative estimation for uniaxially loaded specimens, however, Maximum shear strain criteria provides better results compared to the Brown-Miller criteria. The total strain energy density approach was also used, and both the Masing and non-Masing analysis were adopted in this study. It is found that the Masing model provides conservative fatigue lives, and non-Masing model results in a more realistic fatigue life prediction for 316 LN stainless steel for both low and high strain amplitude. The fatigue design curves obtained from the commonly used analytical low cycle fatigue equations were reexamined for 316 LN SS. The obtained design curves from Langer model and its modified versions are non-conservative for this type of material. Consequently, the authors suggest new optimized parameters to fit the given test data. The obtained curve using the currently suggested parameters is in better agreement with the experimental data for 316 LN SS.


2014 ◽  
Vol 891-892 ◽  
pp. 1320-1326 ◽  
Author(s):  
Thibault Poulain ◽  
José Mendez ◽  
Gilbert Hénaff ◽  
Laurent de Baglion

This paper focuses on the influence of strain rate in Low Cycle Fatigue (LCF) of a 304L austenitic stainless steel at 300 °C in different environments (secondary vacuum, air and Pressurized Water Reactor (PWR) water environment). Moreover test samples are ground to obtain a surface finish rougher than all that could be found in nuclear power plants. Different strain rates (4x10-3, 1x10-4and 1x10-5s-1) are studied, with a triangular waveform at a total strain amplitude of ±0.6%. The influence of strain rate on cyclic stress-strain behavior and fatigue life is firstly analyzed in secondary vacuum, considered as a non-active environment. Then, interactions between stain rate and environmental effects in Air and in PWR environment are presented. In all environments, a decrease in strain rate leads to a negative strain rate dependence of the stress response and a reduction in fatigue life. Finally, SEM observations of fatigue striations in PWR environment indicate a crack propagation rate enhancement when the strain rate is decreased.