Preparation and cyclic oxidation resistance of Hf-doped NiAl coating

2021 ◽  
pp. 110014
Author(s):  
W.L. Zhang ◽  
S.M. Li ◽  
L.B. Fu ◽  
W. Li ◽  
J. Sun ◽  
...  
2013 ◽  
Vol 49 (11) ◽  
pp. 1369 ◽  
Author(s):  
Ziqi GONG ◽  
Ziyong CHEN ◽  
Lihua CHAI ◽  
Zhilei XIANG ◽  
Zuoren NIE

2014 ◽  
Vol 528 ◽  
pp. 25-29
Author(s):  
Ling Yun Bai ◽  
Xian Chao Xu ◽  
Jun Huai Xiang ◽  
Yun Xiang Zheng ◽  
Jun Wang

The cyclic oxidation behavior of Co-10Cr-5Al alloys in atmosphere at 700 °C was investigated. The addition of 0.3 at.% Y changed the oxidation behavior from the approximate parabolic rate law to complex mode. The scale grown on the surface of Co-10Cr-5Al cracked seriously, while the oxide scale the Y doped alloy had better adhesive property. Yttrium doped in the sample promoted the forming of continuous Al2O3layer and decreased the oxidation rate of Co-10Cr-5Al alloys.


2011 ◽  
Vol 148-149 ◽  
pp. 534-537
Author(s):  
Chun Xiang Gao

A very effective approach to improve the oxidation resistance of Ti-6Al-4V alloy was proposed. The Ti-6Al-4V alloy was firstly phosphated and then coated by silica using sol-gel dip-coating technique. A duplex layer of TiP2O7 and amorphous silica was synthesized at the alloy surface. The isothermal and cyclic oxidation behavior of the treated alloy with silica coating and the corresponding bare alloy was investigated at 600 oC in static air to investigate the synergetic effect of phosphorization and amorphous SiO2 coating on the oxidation resistance of the alloy. The isothermal and cyclic oxidation resistances of the alloy were greatly improved.


2009 ◽  
Vol 19 (5) ◽  
pp. 1185-1189 ◽  
Author(s):  
Hong-bo GUO ◽  
Xiao-yan WANG ◽  
Ji LI ◽  
Shi-xing WANG ◽  
Sheng-kai GONG

2014 ◽  
Vol 1015 ◽  
pp. 505-508
Author(s):  
Ling Yun Bai ◽  
Hong Hua Zhang ◽  
Huai Shu Zhang ◽  
Yun Xiang Zheng ◽  
Jun Huai Xiang

The cyclic oxidation behavior of Co-10Cr-5Al alloys with and without 0.3 at% Y doped in atmosphere at 800oC was investigated. The addition of 0.3 at.% Y increased the oxidation rate of the alloy and changed the oxidation mechanism. The scales grown the alloys with and without Y were both composed of an outer Co2O3layer and an inner complex layer of Al2O3, Co2O3and Cr2O3, except that the addition of 0.3 at% Y enhanced the adhesion of the scale. 0.3 at% Y agglomerated in local zone which accelerated the oxidation rate and was not conductive to the oxidation process of the Co-10Cr-5Al alloy.