Dysprosium doped di-strontium magnesium di-silicate white light emitting phosphor by solid state reaction method

Displays ◽  
2014 ◽  
Vol 35 (5) ◽  
pp. 279-286 ◽  
Author(s):  
Ishwar Prasad Sahu ◽  
D.P. Bisen ◽  
Nameeta Brahme
2016 ◽  
Vol 680 ◽  
pp. 228-232
Author(s):  
Xi Guang Gu ◽  
Ren Li Fu ◽  
Ye Tang ◽  
Fang Yang

Ce3+-doped 0.5La2O3-2SrO-0.5Al2O3 (LSA:Ce) phosphors had been successfully synthesized using a conventional solid-state reaction method under reducing atmosphere (H2/N2 =1/5). The phase, morphologies and luminescence properties of the LSA:Ce phosphors were investigated. The emission intensity of LSA:Ce phosphors was improved by the addition of SrF2 as flux, and red shift of PL spectra peak was observed in this phosphors. Research results shown that the LSA:Ce phosphors have the potential to meet the development of white light-emitting diodes.


2015 ◽  
Vol 26 (12) ◽  
pp. 9907-9920 ◽  
Author(s):  
Ishwar Prasad Sahu ◽  
D. P. Bisen ◽  
Nameeta Brahme ◽  
Raunak Kumar Tamrakar ◽  
Ravi Shrivastava

RSC Advances ◽  
2016 ◽  
Vol 6 (3) ◽  
pp. 2368-2373 ◽  
Author(s):  
Cong Zhao ◽  
Da-chuan Zhu ◽  
Ming-jing Tu ◽  
Min Huang ◽  
Ling-ling Peng ◽  
...  

Ce3+ doped aluminosilicate phosphors (Ca2−xAlMg0.5Si1.5O7:xCe3+, x = 0.015–0.075) for white NUV w-LEDs were synthesized by a solid-state reaction method at 1250 °C.


Author(s):  
Yan Zhang ◽  
Yanjie Liang ◽  
Shihai Miao ◽  
Dongxun Chen ◽  
Shao Yan ◽  
...  

A series of Cr3+-doped BaMSi3O9 (M = Zr, Sn, Hf) near-infrared emitting phosphors with tunable luminescence properties have been successfully synthesized by using a simple solid-state reaction method. The developed...


2015 ◽  
Vol 3 (27) ◽  
pp. 7096-7104 ◽  
Author(s):  
Kai Li ◽  
Mengmeng Shang ◽  
Yang Zhang ◽  
Jian Fan ◽  
Hongzhou Lian ◽  
...  

A series of Ca9Bi(PO4)7:Ce3+,Tb3+,Mn2+phosphors synthesizedviathe high-temperature solid-state reaction method can emit intense tunable color from purple-blue to red including white under UV excitation, which shows their potential application in UV-pumped white-light-emitting diodes.


2016 ◽  
Vol 16 (4) ◽  
pp. 3684-3689 ◽  
Author(s):  
Xin Min ◽  
Zhaohui Huang ◽  
Minghao Fang ◽  
Yan’gai Liu ◽  
Chao Tang ◽  
...  

In this paper, M3(VO4)2 (M = Mg, Ca, Sr, and Ba) self-activated phosphors were prepared by a solid-state reaction method at 1,000 °C for 5 h. The phase formation and micrographs were analyzed by X-ray diffraction and scanning electron microscopy. The Ca3(VO4)2 phosphor does not show any emission peaks under excitation with ultraviolet (UV) light. However, the M3(VO4)2 (M = Mg, Sr, and Ba) samples are effectively excited by UV light chips ranging from 200 nm to 400 nm and exhibit broad emission bands due to the charge transfer from the oxygen 2p orbital to the vacant 3d orbital of the vanadium in the VO4. The color of these phosphors changes from yellow to light blue via blue-green with increasing ionic radius from Mg to Sr to Ba. The luminescence lifetimes and quantum yield decrease with the increasing unit cell volume and V–V distance, in the order of Mg3(VO4)2 to Sr3(VO4)2 to Ba3(VO4)2. The emission intensity decreases with the increase of temperatures, but presents no color shift. This confirms that these self-activated M3(VO4)2 phosphors can be suggested as candidates of the single-phase phosphors for light using UV light emitting diodes (LEDs).


2018 ◽  
Vol 12 (1) ◽  
pp. 8-12
Author(s):  
Guo Feng ◽  
Weihui Jiang ◽  
Jianmin Liu ◽  
Cong Li ◽  
Quan Zhang

Novel Eu3+-activated M7Sn(PO4)6 (where M = Sr, Ba) red-emitting phosphors were synthesized via conventional solid-state reaction method at 1200 ?C for 2 h. The luminescence properties of the prepared samples and quenching concentration of Sr7-xSn(PO4)6 :xEu3+ and Ba7-xSn(PO4)6 :xEu3+ were investigated. These phosphors can be efficiently excited by UV (395 nm) and visible blue (465 nm) light nicely matching the output wavelengths of the near-UV LEDs and InGaN blue LED chips and emit the red light. The critical concentrations of the Eu3+ activator were found to be 0.175mol and 0.21mol per formula unit for Sr7-xSn(PO4)6 :xEu3+ and Ba7-xSn(PO4)6 :xEu3+, respectively. The M7-xSn(PO4)6 :xEu3+ (M = Sr, Ba) phosphor may be a good candidate for light-emitting diodes application.