Ba(Ti0.92Sn0.08)O3 lead-free ceramics were prepared using a two-step sintering (TSS) technique. Varying the first sintering temperature T1 (1400 and 1500°C) and the dwell time t1 (0, 15, and 30 min), we obtained dense ceramics which were then soaked at a constant temperature of 1000°C (T2) for 6 h (t2). The structural and electrical properties were investigated. XRD results indicated that all the ceramics showed a pure perovskite phase with tetragonal symmetry. Density and grain size increased with higher T1 temperatures and increased t1 dwell times. Enhanced electrical properties were achieved by sintering at the optimized T1 sintering temperature and t1 dwelling time. At the lower T1 sintering temperature of 1400°C, the dielectric and piezoelectric properties and the Curie temperature of the ceramics were improved significantly by increasing t1 dwell time. Further, increasing the sintering temperature T1 to 1500°C, excellent properties were obtained at t1 = 15 min which then deteriorated when t1 was increased to 30 min. The electrical properties of the sample sintered under the T1/t1/T2/t2 condition of “1500/15/1000/6” showed the best values. For this sample the piezoelectric coefficient (d33), dielectric permittivity (εr), loss factor (tanδ), and Curie temperature (TC) were 490 pC/N, 4385, 0.0272, and 48°C, respectively.


2015 ◽  
Vol 44 (10) ◽  
pp. 4440-4448 ◽  
Author(s):  
Xiang Lv ◽  
Jiagang Wu ◽  
Dingquan Xiao ◽  
Hong Tao ◽  
Yuan Yuan ◽  
...  

In this work, the KNNST-BNKZ-xyz ceramics were obtained, and the composition dependence of their phase structures and electrical properties was discussed.


2019 ◽  
Vol 45 (5) ◽  
pp. 6328-6334 ◽  
Author(s):  
Yunyi Liu ◽  
Yunhe Yi ◽  
Yungang Yu ◽  
Yongqi Pan ◽  
Caiwang He ◽  
...  

2013 ◽  
Vol 479-480 ◽  
pp. 3-7
Author(s):  
Chun Huy Wang

In the present study, various quantities of Bi2O3were added into 0.98(Na0.5K0.5)NbO3-0.02Bi(Na0.93K0.07)TiO3(0.98NKN-0.02BNKT) ceramics. It was found that 0.98NKN-0.02BNKTwith the addition of 0~0.5 wt.% Bi2O3exhibit relatively good piezoelectric properties. For 0.98NKN-0.02BNKT ceramics, the electromechanical coupling coefficients of the planar modekpand the thickness modektreach 0.40 and 0.47,respectively. For 0.98NKN-0.02BNKT ceramics with the addition of 0.3 wt.% Bi2O3, the electromechanical coupling coefficients ofthe planar modekpand the thickness modektreach 0.50 and 0.53, respectively. It is obvious that 0.98NKN-0.02BNKT solid solution ceramics by adding low quantities of Bi2O3is one of the promising lead-free ceramics for electromechanical transducer applications.