Unique defect evolution during the plastic deformation of a metal matrix composite

2019 ◽  
Vol 162 ◽  
pp. 316-320 ◽  
Author(s):  
Yanfang Liu ◽  
Fang Wang ◽  
Yang Cao ◽  
Jinfeng Nie ◽  
Hao Zhou ◽  
...  
MRS Advances ◽  
2015 ◽  
Vol 1 (58) ◽  
pp. 3865-3870 ◽  
Author(s):  
Shima Sabbaghianrad ◽  
Terence G. Langdon

ABSTRACTA severe plastic deformation (SPD) technique was applied to an Al-7075 alloy reinforced with 10 vol.% Al2O3. This processing method of high-pressure torsion (HPT) was performed at room temperature under a pressure of 6.0 GPa through a total number of up to 20 turns. The metal matrix composite (MMC) showed a significant grain refinement from an initial average grain size of ∼8 μm to ∼300 nm after processing by HPT through 20 turns which led to an increase in the average values of Vickers microhardness at room temperature.