Low temperature ferromagnetism in the new diluted magnetic semiconductor p-Bi2$minus;xFexTe3

2003 ◽  
Vol 329-333 ◽  
pp. 1251-1252 ◽  
Author(s):  
V KULBACHINSKII
1989 ◽  
Vol 151 ◽  
Author(s):  
H. J. M. Swagten ◽  
S. J. E. A. Eltink ◽  
W. J. M. De Jonge

ABSTRACTIn this paper experimental evidence is presented for the carrier concentration dependence of the magnetic properties of Sn0.97Mn0.03Te, yielding a critical concentration above which ferromagnetic interactions are dominant. The observed behavior can be fairly well explained within a modified RKKY-model. Preliminary experiments on the low temperature magnetic phases indicate re-entrant spinglass behavior, which is qualitatively described with the spinglass model of Sherrington and Kirkpatrick.


2013 ◽  
Vol 313-314 ◽  
pp. 184-187
Author(s):  
Wen Li Zheng ◽  
Wei Yang

Diluted magnetic semiconductor Zn1-xMnxO crystals were synthesized at 430°C for 24h by hydrothermal method. 3mol·L-1KOH was used as the mineralizer, and the fill factor is 35%. The obtained crystals show a ZnO wurtzite structure, with positive polar faces{0001}, negative polar faces{000 },pfaces{ 011} and–pfaces { 01 } exposed. The height of the crystal is 5-30 m and radius-height ratio is2:1. Mn atom concentration of 2. 6% (x=0.026) was determined using X-ray energy dispersive spectroscopy ( EDS). The crystals show low-temperature ferromagnetism with Curie temperature of 50K.


JETP Letters ◽  
2001 ◽  
Vol 73 (7) ◽  
pp. 352-356 ◽  
Author(s):  
V. A. Kul’bachinskii ◽  
A. Yu. Kaminskii ◽  
K. Kindo ◽  
Y. Narumi ◽  
K. Suga ◽  
...  

2002 ◽  
Vol 312-313 ◽  
pp. 820-822 ◽  
Author(s):  
Jeffrey S. Dyck ◽  
Wei Chen ◽  
Pavel Hájek ◽  
Petr Los̆t’ák ◽  
Ctirad Uher

2001 ◽  
Vol 78 (12) ◽  
pp. 1691-1693 ◽  
Author(s):  
Takashi Hayashi ◽  
Yoshiaki Hashimoto ◽  
Shingo Katsumoto ◽  
Yasuhiro Iye

2012 ◽  
Vol 271-272 ◽  
pp. 26-30
Author(s):  
Wen Li Zheng ◽  
Wei Yang

Diluted magnetic semiconductor Zn1-xMnxO crystals were synthesized at 430°C for 24h by hydrothermal method. 3mol·L-1KOH was used as the mineralizer, and the fill factor is 35%. The obtained crystals show a ZnO wurtzite structure, with positive polar faces{0001}, negative polar faces{000 }, p faces{ 011} and –p faces { 01 } exposed. The height of the crystal is 5-30 m and radius-height ratio is2:1. Mn atom concentration of 2. 6% (x=0.026) was determined using X-ray energy dispersive spectroscopy ( EDS). The crystals show low-temperature ferromagnetism with Curie temperature of 50K.