Supported Fe/MnOx catalyst with Ag doping for remarkably enhanced catalytic activity in Fischer–Tropsch synthesis

2018 ◽  
Vol 8 (7) ◽  
pp. 1953-1970 ◽  
Author(s):  
Yuebing Xu ◽  
Xinli Jia ◽  
Xiaohao Liu

The role of Ag in the promotion of the FTS performance and the evolutions of structure and phase over the Fe/MnOx catalyst has been clearly elucidated.

2021 ◽  
Vol 47 (1) ◽  
pp. 397-418
Author(s):  
Karolina A. Chalupka ◽  
Renata Sadek ◽  
Lukasz Szkudlarek ◽  
Pawel Mierczynski ◽  
Waldemar Maniukiewicz ◽  
...  

Fuel ◽  
2021 ◽  
pp. 122455
Author(s):  
Andrey A. Vasilev ◽  
Mikhail I. Ivantsov ◽  
Ella L. Dzidziguri ◽  
Mikhail N. Efimov ◽  
Dmitry G. Muratov ◽  
...  

2016 ◽  
Vol 6 (12) ◽  
pp. 4594-4600 ◽  
Author(s):  
Geunjae Kwak ◽  
Du-Eil Kim ◽  
Yong Tae Kim ◽  
Hae-Gu Park ◽  
Seok Chang Kang ◽  
...  

In Fischer–Tropsch synthesis (FTS), cobalt carbide (Co2C) is not a catalytically active material, but rather an undesired cobalt phase associated with low catalytic performance.


2020 ◽  
Vol 13 (04) ◽  
pp. 2041001
Author(s):  
Elena Yu. Zakharova ◽  
Anastasiya Yu. Makhaneva ◽  
Maya V. Kulikova ◽  
Maria V. Chudakova ◽  
Mikhail I. Ivantsov ◽  
...  

A series of solid solutions in the PdTe–PdBi system with general formula [Formula: see text]Bix ([Formula: see text], 0.5, 0.67) with the structure based on the NiAs type were synthesized by a high-temperature ampoule technique. These compounds, along with their parent binaries, PdTe and PdBi, were tested as promoters for the standard Co/Al2O3 catalytic system in the Fischer–Tropsch synthesis. It is shown that the addition of PdTe and [Formula: see text]Bix to the standard catalyst increases both yield and selectivity with respect to the liquid phase. At the same time, the addition of PdBi does not only improve catalytic activity, but also slightly inhibits it. Another positive effect of the PdTe and [Formula: see text]Bix addition is the shift in the conversion products toward the diesel and wax fractions. Chemical bonding analysis in orbital and direct space indicates that the addition of Bi to PdTe might increase the localized bonding.


2013 ◽  
Vol 52 (47) ◽  
pp. 12273-12278 ◽  
Author(s):  
David D. Hibbitts ◽  
Brett T. Loveless ◽  
Matthew Neurock ◽  
Enrique Iglesia

2013 ◽  
Vol 634-638 ◽  
pp. 551-554
Author(s):  
Waritsara Bungmek ◽  
Passakorn Kongkinka ◽  
Siwaruk Chotiwan ◽  
Pinsuda Viravathana

The performance of ZrO2-La promoted silica supported cobalt catalyst (100Co/15ZrO2/ 100Aerosil/0.66La) was compared to the ZrO2-Ru promoted one, 100Co/15ZrO2/100Aerosil/0.66Ru, in Fischer-Tropsch synthesis (FTS). These catalysts were prepared by co-precipitation and incipient wetness impregnation methods. The characterization by XRD confirmed the cobalt phase of Co3O4 in both catalysts. For their catalytic activity on FTS reaction, the results preliminarily showed the higher methane fraction (60-80%) and lower C2-C4(10-20%) and C5+(10-20%) fractions in ZrO2-La promoted catalyst compared to the fractions of methane (20-40%), C2-C4(20-50%), and C5+(10-60%) from the ZrO2-Ru promoted catalyst. During reaction, the maximum n-paraffin selectivity of 40% was at C3and the hydrocarbon chain was up to C6for the ZrO2-La promoted catalyst. For the ZrO2-Ru promoted catalyst, the result showed the maximum n-paraffin of C3at 30 min of reaction time. When the reaction time increased, the maximum n-paraffin selectivity shifted toward higher C number but levelled off (15%) and the hydrocarbon chain was up to C16.


2016 ◽  
Vol 337 ◽  
pp. 260-271 ◽  
Author(s):  
Kang Cheng ◽  
Vijayanand Subramanian ◽  
Alexandre Carvalho ◽  
Vitaly V. Ordomsky ◽  
Ye Wang ◽  
...  