Experimental study of the Mode I adhesive fracture energy in DCB specimens bonded with a polyurethane adhesive

2015 ◽  
Vol 93 (3) ◽  
pp. 235-255 ◽  
Author(s):  
Yu Sekiguchi ◽  
Masato Katano ◽  
Chiaki Sato
2006 ◽  
Vol 20 (10) ◽  
pp. 1109-1124 ◽  
Author(s):  
S. B. Kumar ◽  
I. Sridhar ◽  
S. Sivashanker ◽  
S. O. Osiyemi

2020 ◽  
Vol 8 (1) ◽  
Author(s):  
Jyotikalpa Bora ◽  
Sushen Kirtania

Abstract A comparative study of elastic properties and mode I fracture energy has been presented between conventional carbon fibre (CF)/epoxy and advanced carbon nanotube (CNT)/epoxy laminated composite materials. The volume fraction of CNT fibres has been considered as 15%, 30%, and 60% whereas; the volume fraction of CF has been kept constant at 60%. Three stacking sequences of the laminates viz.[0/0/0/0], [0/90/0/90] and [0/30/–30/90] have been considered in the present analysis. Periodic microstructure model has been used to calculate the elastic properties of the laminated composites. It has been observed analytically that the addition of only 15% CNT in epoxy will give almost the same value of longitudinal Young’s modulus as compared to the addition of 60% CF in epoxy. Finite element (FE) analysis of double cantilever beam specimens made from laminated composite has also been performed. It has been observed from FE analysis that the addition of 15% CNT in epoxy will also give almost the same value of mode I fracture energy as compared to the addition of 60% CF in epoxy. The value of mode I fracture energy for [0/0/0/0] laminated composite is two times higher than the other two types of laminated composites.


Holzforschung ◽  
2002 ◽  
Vol 56 (2) ◽  
pp. 191-198 ◽  
Author(s):  
Alexander Reiterer ◽  
Gerhard Sinn

Summary The fracture properties of unmodified and modified (heat treatments under various conditions and acetylation) sprucewood are investigated using the wedge splitting test. Fracture parameters measured include critical stress intensity factor and specific fracture energy under Mode I loading and specific fracture energy under Mode III loading. The Mode I fracture properties are reduced by all kinds of modification. However, acetylation leads to a reduction of only 20%whereas heat treatments reduce the properties to a much greater extent, approximately 50%to 80%. The Mode III fracture properties are influenced less. SEM pictures of the fracture surfaces support the described findings.


Sign in / Sign up

Export Citation Format

Share Document