Nano-Mechanical and Corrosion Properties of Cold Rolled Duplex Stainless Steel Sheet with 0.1 wt.% Gadolinium

2017 ◽  
Vol 9 (1) ◽  
pp. 74-76 ◽  
Author(s):  
Youl Baik ◽  
Yong Choi ◽  
Byung Moon Moon
2015 ◽  
Vol 116 (11) ◽  
pp. 1135-1142 ◽  
Author(s):  
Youl Baik ◽  
Yong Choi ◽  
Byung M. Moon ◽  
Dong S. Sohn ◽  
S. G. Bogdanov ◽  
...  

2005 ◽  
Vol 495-497 ◽  
pp. 363-368
Author(s):  
Soo Ho Park ◽  
Hyung Gu Kang ◽  
Yong Deuk Lee ◽  
Jae Chul Lee ◽  
Moo Young Huh

In order to investigate the effect of the reduction degree per rolling pass on the evolution of recrystallization textures and microstructures, the hot band of 17.5 Cr-1.1 Mo ferritic stainless steel sheets were cold rolled with lubrication according to two processing routes, by which different reduction degrees per pass were introduced. Rolling with a large number of passes led to the formation of fairly homogeneous rolling textures at all through-thickness positions. In contrast, cold rolling with large draughts resulted in pronounced texture gradients along the thickness direction. After recrystallization annealing, the texture maximum was obtained at {334}<483> in all samples regardless of the rolling routes and thickness layers. During subsequent annealing, recrystallization was observed to be faster in those grains with {111}<uvw> orientations, while it was retarded in grains having orientations close to {001}<110>.


2004 ◽  
Vol 75 (12) ◽  
pp. 829-835 ◽  
Author(s):  
Daniel Krizan ◽  
Lode Duprez ◽  
Bruno C. De Cooman

2021 ◽  
Vol 63 (9) ◽  
pp. 791-796
Author(s):  
Lei Tian ◽  
Zhanqi Gao ◽  
Yongdian Han

Abstract To investigate the influence of post-weld heat treatment on the microstructure and corrosion properties of super duplex stainless steel welded joints, multi-layer multi-pass welding of 2507 super duplex stainless steel by tungsten argon arc welding was performed using an ER2594 welding wire. The microstructures of the welded joints before and after post-weld heat treatment at 1150 °C, 1170 °C and 1190 °C were observed, and the mechanical and corrosion properties were tested. The post-weld heat treatment changed the austenite content and morphology of the welded joint and improved the corrosion resistance of different parts of the weld metal. The choice of various solution heat treatment temperatures affected the change in austenite content in the weld zone and the degree of diffusion and homogenization of the alloy elements. After post-weld heat treatment at 1170 °C, the two-phase ratios in each area of the weld were the most suitable and uniform, and the overall mechanical and corrosion properties of the joint were more uniform.


2004 ◽  
Vol 467-470 ◽  
pp. 217-222 ◽  
Author(s):  
R. Badji ◽  
B. Belkessa ◽  
H. Maza ◽  
M. Bouabdallah ◽  
Brigitte Bacroix ◽  
...  

Duplex stainless steels 2205 are widely used in constructional and petrochemical applications because of their good mechanical and corrosion properties. The objective of this work was to study the influence of aging at high temperature on the austenite and d ferrite equilibrium. After welding by TIG process, duplex stainless steel was aged in the range of 800 – 1150 °C temperatures for 60 min. The microstructure was characterized by metallography and X-ray methods. The toughness of welded structure was also measured.