scholarly journals Магнитные взаимодействия в структуре фазы Ауривиллиуса Bi-=SUB=-5-=/SUB=-FeTi-=SUB=-3-=/SUB=-O-=SUB=-15-=/SUB=-

2022 ◽  
Vol 64 (2) ◽  
pp. 213
Author(s):  
С.Г. Ястребов ◽  
Н.А. Ломанова

This paper analysis the temperature dependence of FC and ZFC magnetization for Bi5FeTi3O15 multiferroic. It has Aurivillius four-layer phase structure. The analysis evidence on the influence of the grains of this material on its overall magnetic properties. The lack of a dramatic temperature threshold in the FC(ZFC) dependences may result in spin canting induced by the Dzyaloshinskii-Moriya interaction.

2021 ◽  
Vol 214 (1) ◽  
pp. 56-68
Author(s):  
Surirat Yotthuan ◽  
Siradanai Rueanngam ◽  
Supree Pinitsoontorn ◽  
Suphornphun Chootin ◽  
Theerachai Bongkarn

2009 ◽  
Vol 321 (5) ◽  
pp. 438-441 ◽  
Author(s):  
Lezhong Li ◽  
Zhongwen Lan ◽  
Zhong Yu ◽  
Ke Sun ◽  
Ming Luo ◽  
...  

Materials ◽  
2021 ◽  
Vol 14 (10) ◽  
pp. 2526
Author(s):  
Grzegorz Ziółkowski ◽  
Artur Chrobak ◽  
Ewa Talik ◽  
Joanna Klimontko ◽  
Dariusz Chrobak

This paper refers to the structural and magnetic properties of [(Fe80Nb6B14)0.88Dy0.12]1−xZrx (x = 0; 0.01; 0.02; 0.05; 0.1; 0.2; 0.3; 0.5) alloys obtained by the vacuum mold suction casting method. The analysis of the phase contribution indicated a change in the compositions of the alloys. For x < 0.05, occurrence of the dominant Dy2Fe14B phase was observed, while a further increase in the Zr content led to the increasing contribution of the Fe–Zr compounds and, simultaneously, separation of crystalline Dy. The dilution of (Fe80Nb6B14)0.88Dy0.12 in Zr strongly influenced the magnetization processes of the examined alloys. Generally, with the increasing x parameter, we observed a decrease in coercivity; however, the unexpected increase in magnetic saturation and remanence for x = 0.2 and x = 0.3 was shown and discussed.


2018 ◽  
Vol 30 (3) ◽  
pp. 2809-2820
Author(s):  
Peng-zhao Gao ◽  
Zhi-bo Huang ◽  
Hang-bo Zheng ◽  
Xiao-pan Liu ◽  
Jin Wen ◽  
...  

2021 ◽  
Author(s):  
Andrey Malyshev ◽  
Anna B. Petrova ◽  
Anatoly P. Surzhikov

Abstract The effect of the diamagnetic ZrO2 addition on the microstructure and magnetic properties of LiTiZn ferrite ceramics, including the shape and parameters of the temperature dependence of the initial permeability, has been investigated. The defect structure of ferrite ceramic samples is assessed according to our earlier proposed method based on mathematical treatment of the experimental temperature dependencies of the initial permeability. The method is recommended for defects monitoring of soft ferrite ceramics and ferrite products. It was found that the defect structure of ferrite ceramics increased by 350% with an increase in the concentration of the ZrO2 additive in the range of (0–0.5) wt.%. In this case, for the same samples, the increase in the true physical broadening of reflections is only 20%, and the coercive force by 50%. Simultaneously, the maximum of the experimental temperature dependence of the initial permeability dropped by 45%. The microstructure of all samples is characterized with a similar average grain size according to the SEM data. However, samples with the 0.5wt.% of ZrO2 are characterized by the formation of conglomerates. A linear relationship was obtained between the defect structure and the width of the reflections, which indicates that this parameter is related to the elastic stress of ferrite ceramics.


2011 ◽  
Vol 120 (6) ◽  
pp. 1070-1073 ◽  
Author(s):  
N. Guskos ◽  
S. Glenis ◽  
G. Zolnierkiewicz ◽  
J. Typek ◽  
D. Sibera ◽  
...  

1994 ◽  
Vol 132 (1-3) ◽  
pp. 153-158 ◽  
Author(s):  
R.V. Mehta ◽  
R.V. Upadhyay ◽  
B.A. Dasannacharya ◽  
P.S. Goyal ◽  
K.S. Rao

1999 ◽  
Vol 13 (29n31) ◽  
pp. 3528-3531
Author(s):  
J. JUNG ◽  
H. YAN ◽  
H. DARHMAOUI ◽  
M. ABDELHADI

We have found the correlation between nanoscopic phase separation in the copper-oxygen planes of YBCO and TlBCCO and the transport and magnetic properties of these materials in the a-b planes such as: the temperature dependence of the critical current density Jc( T ), the temperature dependence of the superfluid density ns( T )∝1/λ2( T ) at low temperatures, the temperature dependence of the normalized logarithmic relaxation rate S(T), and the dependence of the effective energy barrier against vortex motion on the current density Ueff( J ). These properties are controlled by the ratio of the amount of an underdoped filamentary phase to that of an optimally doped one.


2021 ◽  
pp. 1-1
Author(s):  
Wenting Zhang ◽  
Qingxin Yang ◽  
Yongjian Li ◽  
Zhiwei Lin ◽  
Ming Yang

Sign in / Sign up

Export Citation Format

Share Document