scholarly journals Polymers Sorption Properties towards Photosynthetic Pigments and Fungicides

Materials ◽  
2021 ◽  
Vol 14 (8) ◽  
pp. 1874
Author(s):  
Małgorzata Tatarczak-Michalewska ◽  
Jolanta Flieger ◽  
Justyna Kawka ◽  
Wojciech Płaziński ◽  
Tomasz Klepka ◽  
...  

In the present work, extraction with a solvent (cold acetone) was used to extract the assimilation pigments from spinach leaves. Then, the sorption capacity of selected plastics granules (polyvinyl chloride—PVC, polypropylene—PP, polyethylene—PE of different densities) was tested for the selective isolation of chlorophylls. Quantification of chlorophylls by HPLC (Zorbax Eclipse XDB-C18 column, the mobile phase: Acetonitrile/methanol/ethyl acetate 6:2:2, v/v) was based on chlorophyll-a content as the most common chlorophyll. The performed experiments prove that PVC containing electronegative chlorine exhibits favorable interactions toward chlorophyll by creating stable molecular complexes. The Fourier Transform Raman Spectroscopy (FT-Raman) and the molecular modeling were used to elucidate the structure of the created complexes. The optimal extraction requirements, the mass of sorbent, water-acetone ratio, time, and the composition of the elution solvent were all established. The optimized extraction conditions ensured a maximum extraction yield of chlorophylls of 98%. The chlorophyll-rich sorbent was re-extracted by acetone, leading to the recovery of 91% of chlorophylls in one step, adding the possibility of its re-use. The proposed effective and ecological method of obtaining the green dye from plants is cheap, simple, and efficient, avoiding organic solvents, utilizing the most widely used synthetic polymers in the world, being products difficult for utilization. The possibility to remove chosen fungicides cyprodinil, chlorothalonil, and thiabendazone from plant extract by PVC was also examined. The described method proposes a new application of synthetic polymers, which meets the criteria of sustainable green chemistry, simultaneously reaching the growing demand for pure natural compounds in the pharmaceutical and food industries.

Clay Minerals ◽  
1997 ◽  
Vol 32 (1) ◽  
pp. 65-77 ◽  
Author(s):  
R. L. Frost

AbstractThe Fourier transform Raman spectra of the kaolinite minerals have been measured in the 50–3800 cm−1 region using near infrared spectroscopy. Kaolinites are characterized by remarkably intense bands in the 120–145 cm−1 region. These bands, attributed to the O-Si-O and O-Al-O symmetric bending modes, are both polymorph and orientation dependent. The 200–1200 cm−1 spectral range is a finger-print region for clay minerals and each kaolinite clay has its own characteristic spectrum. The structure of clays is fundamentally determined by the position of hydroxyl groups. Fourier-transform Raman spectroscopy readily enables the hydroxyl stretching region to be examined allowing identification of the component bands. The advantages of FT-Raman spectroscopy are shown to enhance the study of the kaolinite structure.


Materials ◽  
2021 ◽  
Vol 14 (11) ◽  
pp. 3138
Author(s):  
Kamila Gosz ◽  
Agnieszka Tercjak ◽  
Adam Olszewski ◽  
Józef Haponiuk ◽  
Łukasz Piszczyk

The utilization of forestry waste resources in the production of polyurethane resins is a promising green alternative to the use of unsustainable resources. Liquefaction of wood-based biomass gives polyols with properties depending on the reagents used. In this article, the liquefaction of forestry wastes, including sawdust, in solvents such as glycerol and polyethylene glycol was investigated. The liquefaction process was carried out at temperatures of 120, 150, and 170 °C. The resulting bio-polyols were analyzed for process efficiency, hydroxyl number, water content, viscosity, and structural features using the Fourier transform infrared spectroscopy (FTIR). The optimum liquefaction temperature was 150 °C and the time of 6 h. Comprehensive analysis of polyol properties shows high biomass conversion and hydroxyl number in the range of 238–815 mg KOH/g. This may indicate that bio-polyols may be used as a potential substitute for petrochemical polyols. During polyurethane synthesis, materials with more than 80 wt% of bio-polyol were obtained. The materials were obtained by a one-step method by hot-pressing for 15 min at 100 °C and a pressure of 5 MPa with an NCO:OH ratio of 1:1 and 1.2:1. Dynamical-mechanical analysis (DMA) showed a high modulus of elasticity in the range of 62–839 MPa which depends on the reaction conditions.


1991 ◽  
Vol 7 (Supple) ◽  
pp. 415-418 ◽  
Author(s):  
Norio TERAMAE ◽  
Takumi ANDO ◽  
Shigeru UCHIJIMA ◽  
Hiroki HARAGUCHI ◽  
Masahide NOJI

1989 ◽  
Vol 164 (2-3) ◽  
pp. 178-184 ◽  
Author(s):  
P.J. Hendra ◽  
C. Passingham ◽  
G.M. Warnes ◽  
R. Burch ◽  
D.J. Rawlence