Enhanced wetting behavior using femtosecond laser-textured surface in laser welding-brazing of Ti/Al butt joint

2021 ◽  
Vol 142 ◽  
pp. 107212
Author(s):  
Xi Chen ◽  
Zhenglong Lei ◽  
Yanbin Chen ◽  
Meng Jiang ◽  
Nan Jiang ◽  
...  
2021 ◽  
Vol 18 (9) ◽  
pp. 096002
Author(s):  
Hua Tan ◽  
Jiahui Pan ◽  
Xiaojia Zheng ◽  
Xiaoquan Fu

SciVee ◽  
2012 ◽  
Author(s):  
Ivo Lenzetti ◽  
Alex Malandrini ◽  
Annalisa Canovetti ◽  
Luca Menabuoni ◽  
Francesca Rossi ◽  
...  

2011 ◽  
Vol 38 (6) ◽  
pp. 0603013
Author(s):  
陈根余 Chen Genyu ◽  
陈飞 Chen Fei ◽  
张屹 Zhang Yi ◽  
李时春 Li Shichun ◽  
康斌 Kang Bin

2020 ◽  
Vol 47 (9) ◽  
pp. 0902005
Author(s):  
于淼 Yu Miao ◽  
黄婷 Huang Ting ◽  
肖荣诗 Xiao Rongshi

2019 ◽  
Vol 6 (9) ◽  
pp. 096533
Author(s):  
Xiaoquan Yu ◽  
Ding Fan ◽  
Jiankang Huang ◽  
Yutao Kang

2019 ◽  
Vol 14 (1) ◽  
Author(s):  
Huan Yang ◽  
Kaichen Xu ◽  
Changwen Xu ◽  
Dianyuan Fan ◽  
Yu Cao ◽  
...  

Abstract Highly stretchable and robust superhydrophobic surfaces have attracted tremendous interest due to their broad application prospects. In this work, silicone elastomers were chosen to fabricate superhydrophobic surfaces with femtosecond laser texturing method, and high stretchability and tunable adhesion of the superhydrophobic surfaces were demonstrated successfully. To our best knowledge, it is the first time flexible superhydrophobic surfaces with a bearable strain up to 400% are fabricated by simple laser ablation. The test also shows that the strain brings no decline of water repellency but an enhancement to the superhydrophobic surfaces. In addition, a stretching-induced transition from “petal” state to “lotus” state of the laser-textured surface was also demonstrated by non-loss transportation of liquid droplets. Our results manifest that femtosecond laser ablating silicone elastomer could be a promising way for fabricating superhydrophobic surface with distinct merits of high stretchability, tunable adhesion, robustness, and non-fluorination, which is potentially useful for microfluidics, biomedicine, and liquid repellent skin.


2017 ◽  
Vol 118 ◽  
pp. 53-65 ◽  
Author(s):  
Junhao Sun ◽  
Kai Feng ◽  
Ke Zhang ◽  
Baochao Guo ◽  
En Jiang ◽  
...  

2015 ◽  
Vol 1114 ◽  
pp. 272-277 ◽  
Author(s):  
Alexandru Ghiban ◽  
Mihai Buzatu ◽  
Cristina Maria Bortun ◽  
Brandusa Ghiban ◽  
Nicolae Serban

Optimization of fractured or destroyed removable partial dentures realized from CoCrMo alloys are possible due to modern welding equipments. The aim of study was to offer the processing and welding optimal parameters for some long lasting prosthetic pieces. There are investigated two cobalt based alloys, used for dental applications, types CoCrMo. Laser welding equipments was a Mini Laser XXS (Orotig Italia) and the tested samples were welded in butt joint, without filler material. There are presented in comparison results concerning macro and micro structural analysis made on stereomicroscope OLYMPUS and Reichert microscope. Finally a correlation between different welding parameter values and structural features was made.


Sign in / Sign up

Export Citation Format

Share Document