Comparison of the Trueness of Fits of the Biphasic Transverse Isotropic and Kelvin Models to the Tensile Behavior of Temporomandibular Joint Disc

2021 ◽  
Vol 143 (6) ◽  
Author(s):  
Wuyang Li ◽  
Sara Trbojevic ◽  
Alejandro J. Almarza

Abstract This technical brief explores the validity and trueness of fit for using the transverse isotropic biphasic and Kelvin models (first and second order generalized) for characterization of the viscoelastic tensile properties of the temporomandibular joint (TMJ) discs from pigs and goats at a strain rate of 10 mm/min. We performed incremental stress-relaxation tests from 0 to 12% strain, in 4% strain steps on pig TMJ disc samples. In addition, to compare the outcomes of these models between species, we also performed a single-step stress-relaxation test of 10% strain. The transverse isotropic biphasic model yielded reliable fits in reference to the least root mean squared error method only at low strain, while the Kelvin models yielded good fits at both low and high strain, with the second order generalized Kelvin model yielding the best fit. When comparing pig to goat TMJ disc in 10% strain stress-relaxation test, unlike the other two Kelvin models, the transverse isotropic model did not fit well for this larger step. In conclusion, the second order Kelvin model showed the best fits to the experimental data of both species. The transverse isotropic biphasic model did not fit well with the experimental data, although better at low strain, suggesting that the assumption of water flow only applies while uncrimping the collagen fibers. Thus, it is likely that the permeability from the biphasic model is not truly representative, and other biphasic models, such as the poroviscoelastic model, would likely yield more meaningful outputs and should be explored in future works.

2016 ◽  
Vol 853 ◽  
pp. 158-162
Author(s):  
Jie Zhao ◽  
Tie Shan Cao ◽  
Cong Qian Cheng ◽  
Hui Fang Li

The current paper investigates on the creep behavior of 12Cr-Mo-W-0.25V heat resistant steel base on the long-term stress relaxation test data. It is shows that the stress relaxation curve can be divided into 2 stages: the high stress stage has higher apparent activation volume of 79~350 b3 and the low stress stage is 35~78 b3. Besides, the Helmholtz free energy at the high stress stage is 827~1034 kJ/mol which is higher than 210~252 kJ/mol of the low stress stage. Taking both apparent activation volume and activation energy into account, it is assumed that the high stress stage is mainly controlled by dislocation slip and the low stress stage is more related to diffusion.


2014 ◽  
Vol 563 ◽  
pp. 48-52
Author(s):  
Lei Chen ◽  
Zhi Xin Yu ◽  
Wei Ping Cui ◽  
Li Juan Qin

Development of normal stress in the direction perpendicular to the asphalt mixture is an important feature of the nonlinear viscoelastic behavior of asphalt binders. In this paper, this phenomenon was studied with the help of stress-relaxation experiments in torsion.  Results indicate that stress relaxation test by controlling strain could be used to evaluate the stress relaxation ability of asphalt mixture. With the aging degree of asphalt mixtures increased, the low temperature cracking resistance got worse; the higher the temperature is, the faster the stress relaxed; the smaller the initial strain, the worse the stress relaxation ability also. The viscoelasticity of asphalt mixture could be simulated by exponential model fractional and the experiments well supported the modeling results.


Sign in / Sign up

Export Citation Format

Share Document