Construction of Al-based solid-solution range boundaries in the Al-Sc-Si system at 550 and 500°C

2011 ◽  
Vol 2011 (11) ◽  
pp. 1064-1068 ◽  
Author(s):  
A. V. Sukhanov ◽  
L. L. Rokhlin ◽  
N. R. Bochvar
2001 ◽  
Vol 691 ◽  
Author(s):  
Ichiro Matsubara ◽  
Ryoji Funahashi ◽  
Masahiro Shikano ◽  
Kei Sasaki ◽  
Hiroyuki Enomoto

ABSTRACTWe have prepared (Ca1−x−yMxBiy)3Co4Oz (M = Mg, Sr, and Ba) thin films by a combinatorial approach using a solution process. In the systems of (Ca1−x−yMxBiy)3Co4Oz (M = Mg, Sr, and Ba), solid solution range was determined to be × < 0.8 (M = Sr, y = 0), x < 1.0 (M = Mg, y = 0), x = 0.0 (M = Ba, y = 0), and x < 0.4 (M = Bi, x = 0). No solid solution range was obtained for the substitution of Ba for Ca site. The in-plane compressive stress in the CoO2 sublattice is controllable by the cation substitution for Ca in the (Ca2CoO3) sublattice. With increasing in-plane stress, the magnitude of thermoelectric power and resistivity increased.


1997 ◽  
Vol 17 (4) ◽  
pp. 575-580 ◽  
Author(s):  
Lars-Olov Nordberg ◽  
Zhijian Shen ◽  
Mats Nygren ◽  
Thommy Ekström

2002 ◽  
Vol 335 (1-2) ◽  
pp. 191-195 ◽  
Author(s):  
Toetsu Shishido ◽  
Takahiko Sasaki ◽  
Kunio Kudou ◽  
Shigeru Okada ◽  
Akira Yoshikawa ◽  
...  

1997 ◽  
Vol 171 (3-4) ◽  
pp. 458-462 ◽  
Author(s):  
Satoshi Uda ◽  
Ryuichi Komatsu ◽  
Kouichi Takayama

1996 ◽  
Vol 11 (4) ◽  
pp. 268-275 ◽  
Author(s):  
Winnie Wong-Ng ◽  
F. Jiang ◽  
Bryan R. Jarabek ◽  
Gregory J. McCarthy

Powder X-ray diffraction was used to investigate the solid solution range of the Bi14SrxCa12−xO33 series in the Bi–Sr–Ca–O system. Solid solution forms over the range 1≤x≤7 in Bi14SrxCa12−xO33. Experimental X-ray reference patterns of selected members with x=1, 3, 5, and 7 have been prepared for the powder diffraction file (PDF). These phases are monoclinic, C2/m, with cell parameter a ranging from 21.473(4) to 21.868(4) Å, b from 4.3564(9) to 4.3898(9) Å, c from 12.753(2) to 12.962(2) Å, β from 102.91(2)° to 102.79(1)°, and V from 1162.9(3) to 1213.5(3) Å3, respectively. These parameters increase monotonically as Ca is continuously replaced by the larger Sr.


2008 ◽  
Vol 155 (11) ◽  
pp. A866 ◽  
Author(s):  
Uday S. Kasavajjula ◽  
Chunsheng Wang ◽  
Pedro E. Arce

1999 ◽  
Vol 291 (1-2) ◽  
pp. 52-56 ◽  
Author(s):  
Toetsu Shishido ◽  
Jinhua Ye ◽  
Kunio Kudou ◽  
Shigeru Okada ◽  
Kazuo Obara ◽  
...  

Sign in / Sign up

Export Citation Format