Mechanical properties of (Bi,Sb)2Te3 solid solutions obtained by directional crystallization and spark plasma sintering

2016 ◽  
Vol 42 (1) ◽  
pp. 105-107 ◽  
Author(s):  
M. G. Lavrent’ev ◽  
V. B. Osvenskii ◽  
G. I. Pivovarov ◽  
A. I. Sorokin ◽  
L. P. Bulat ◽  
...  
2019 ◽  
Vol 30 ◽  
pp. 411-418
Author(s):  
Ojo Jeremiah Akinribide ◽  
Gadifele Nicolene Mekgwe ◽  
Olawale Olarewaju Ajibola ◽  
Babatunde Abiodun Obadele ◽  
Samuel Olukayode Akinwamide ◽  
...  

2014 ◽  
Vol 40 (7) ◽  
pp. 10517-10522 ◽  
Author(s):  
Shaocun Liu ◽  
Wentao Hu ◽  
Jianyong Xiang ◽  
Fusheng Wen ◽  
Bo Xu ◽  
...  

2014 ◽  
Vol 616 ◽  
pp. 52-55 ◽  
Author(s):  
Ying Li ◽  
Hirokazu Katsui ◽  
Takashi Goto

Titanium carbide (TiC) was consolidated with 20 mol% zirconium carbide (ZrC) by spark plasma sintering in the temperature range of 1773–2473 K, and the phase formation, microstructure, relative density and mechanical properties were investigated. The composite consisted of Ti-rich (Ti, Zr)C and Zr-rich (Zr, Ti)C solid solutions at 1773–2373 K, and was single-phase (Ti, Zr)C at 2473 K. The relative density of the composite was over 98% above 2073 K. The composite prepared at 2273 K exhibited the maximumHVof 29.7 GPa with theKICof 3.76 MPa m1/2.


2011 ◽  
Vol 49 (01) ◽  
pp. 40-45 ◽  
Author(s):  
Hyun-Kuk Park ◽  
Seung-Min Lee ◽  
Hee-Jun Youn ◽  
Ki-Sang Bang ◽  
Ik-Hyun Oh

2021 ◽  
Vol 63 (9) ◽  
pp. 1583-1589
Author(s):  
D. A. Osipov ◽  
I. V. Smirnov ◽  
K. V. Grinyaev ◽  
I. A. Ditenberg ◽  
M. A. Korchagin