Cut Fe 40 Ni 38 B 18 Mo 4 ribbons were annealed for two hours at various temperatures Ta between 400 and 540°C. All the ribbons were subjected to XRD, VSM (vibrating sample magnetometer) and ME (Mossbauer effect spectroscopy) investigations. A differential thermal analysis scan of an as-cast ribbon showed the presence of two exothermic peaks, the first beginning at 419.9°C and peaking at 429.7°C and the second beginning at 497.3°C and ending at 546.2°C. The XRD patterns of the ribbons showed the formation of FeNi 3 nanocrystallites in the lower T'a ribbons and (Fe, Ni, Mo) 23 B 6 crystallites in the ribbons annealed above 470°C. Different behaviors of the saturation magnetization were seen in the ribbons annealed between 400 and 450°C, between 450 and 490°C, and between 490 and 540°C. The ME spectra of the ribbons annealed in the three different temperature ranges also pointed to the presence of three crystalline Fe-compounds in these ranges. The XRD patterns and the coercivities (Hc) of the lower Ta ribbons point to the formation of nanocrystallites in these ribbons.

2010 ◽  
Vol 158 ◽  
pp. 52-55 ◽  
Author(s):  
Ye Han ◽  
Ming Gu ◽  
Wei Wei Zhang ◽  
Shu Yu Yao

The Fe2O3-CaO-SiO2 glass ceramics were prepared by the method of quenching and controlled crystallisation. Differential thermal analysis, X-ray diffractometry and vibrating sample magnetometer were used to study the crystallisation and magnetic properties of Fe2O3-CaO-SiO2 glass ceramics. It was concluded that the main crystalline phases of glass ceramics during the process were Hematite, Iron Silico Oxide and Hedenbergite. The saturation magnetisation values (Ms) of glass ceramics varied between 108 emu•g-1 and 147 emu•g-1. The crystallisation of Hedenbergite lead to the high Hc value (~2000Oe).


1973 ◽  
Vol 58 (10) ◽  
pp. 4610-4613 ◽  
Author(s):  
J. A. Cameron ◽  
L. Keszthelyi ◽  
G. Nagy ◽  
L. Kacsóh

1982 ◽  
Vol 10 (3) ◽  
pp. 325-332 ◽  
Author(s):  
D. Scherson ◽  
S.B. Yao ◽  
E.B. Yeager ◽  
J. Eldridge ◽  
M.E. Kordesch ◽  
...  

2010 ◽  
Vol 160-162 ◽  
pp. 1787-1790
Author(s):  
Jing Cao ◽  
Yong Feng Wang ◽  
Chun Xue Wei

1J79 alloy was prepared by vacuum electric arc smelting.The crystal growth and the content of impurity was observed by electron probe microanalyzer,and magnetic properties were measured by vibrating sample magnetometer(VSM).Experimental results show that inclusions in the alloy are fewer and fewer, composition becomes more uniform with the increases of the Mo content, and grain size also becomes larger and larger with the increases of Mo content, to reduce coercivity. The small amount of Mo addition is useful to improve the saturation magnetization and reduce coercivity.


1982 ◽  
Vol 53 (3) ◽  
pp. 2377-2379 ◽  
Author(s):  
Chen Ming‐Yan ◽  
Wang Hui‐Juan ◽  
Yan Yong ◽  
Shao Han‐Ru ◽  
Li De‐Xin ◽  
...  

1984 ◽  
Vol 86 (2) ◽  
pp. 655-662 ◽  
Author(s):  
H. M. van Noort ◽  
D. B. De Mooij ◽  
K. H. J. Buschow

1974 ◽  
Vol 9 (4) ◽  
pp. 537-543 ◽  
Author(s):  
Y. Takeda ◽  
M. Shimada ◽  
F. Kanamaru ◽  
M. Koizumi ◽  
N. Yamamoto

1995 ◽  
Vol 146 (1-2) ◽  
pp. 123-128 ◽  
Author(s):  
D.P. Middleton ◽  
F.M. Mulder ◽  
R.C. Thiel ◽  
K.H.J. Buschow