Since pipe bend has a characteristic that extrados becomes thinner and intrados thicker after fabrication process, it can be expected to be vulnerable to extrados wall thinning due to corrosion or erosion during its operation. In this paper, limit loads of pipe bend with the thinning are computed under the loading conditions of internal pressure and bending moment. Several case studies with varying geometries and wall thinning shapes are presented. The difference in the limit loads behavior between pipe bend and welded elbow is also reviewed. The calculated plastic limit loads of pipe bend are compared with other research results for the welded elbow. The results show that pipe bend can be applied to safety-related piping systems as far as the internal pressure and bending moment only are considered.


2017 ◽  
Vol 62 (3) ◽  
pp. 1881-1887
Author(s):  
P. Ramaswami ◽  
P. Senthil Velmurugan ◽  
R. Rajasekar

Abstract The present paper makes an attempt to depict the effect of ovality in the inlet pigtail pipe bend of a reformer under combined internal pressure and in-plane bending. Finite element analysis (FEA) and experiments have been used. An incoloy Ni-Fe-Cr B407 alloy material was considered for study and assumed to be elastic-perfectly plastic in behavior. The design of pipe bend is based on ASME B31.3 standard and during manufacturing process, it is challenging to avoid thickening on the inner radius and thinning on the outer radius of pipe bend. This geometrical shape imperfection is known as ovality and its effect needs investigation which is considered for the study. The finite element analysis (ANSYS-workbench) results showed that ovality affects the load carrying capacity of the pipe bend and it was varying with bend factor (h). By data fitting of finite element results, an empirical formula for the limit load of inlet pigtail pipe bend with ovality has been proposed, which is validated by experiments.


Author(s):  
Andrew Cosham ◽  
Robert Andrews

Abstract Annex G Assessment of locally thinned areas (LTAs) in BS 7910:2013 is applicable to LTAs in cylinder, a bend and a sphere or vessel end. It can be used to assess the longitudinally-orientated LTA in a cylinder subject to a hoop stress and a circumferentially-orientated LTA in a cylinder subject to an axial stress (due to axial force, in-plane bending moment and internal pressure), and also to assess an LTA subject to a hoop stress and an axial stress. An outline of the origins of Annex G is given. A comparison with full-scale burst tests of pipes or vessels containing LTAs subject to a hoop stress and an axial stress is presented. It is demonstrated that the method in G.4.3 Hoop stress and axial stress is conservative.


Author(s):  
Tarek M. A. A. EL-Bagory ◽  
Maher Y. A. Younan ◽  
Hossam E. M. Sallam ◽  
Lotfi A. Abdel-Latif

The aim of this paper is to investigate the effect crack depth a/W = 0 to 0.4 and load angle (30°,45°,and 60°) on the limit load of miter pipe bends (MPB) under out-of-plane bending moment with a crosshead speed 500 mm/min. The geometry of cracked and uncracked multi miter pipe bends are: bend angle, α = 90°, pipe bend factor, h = 0.844, standard dimension ratio, SDR = 11, and three junctions, m = 3. The material of the investigated pipe is a high-density polyethylene (HDPE), which is applied in natural gas piping systems. Butt-fusion welding is used to produce the welds in the miter pipe bends. An artificial crack is produced by a special cracking device. The crack is located at the crown side of the miter pipe bend, such that the crack is collinear with the direction of the applied load. The crack depth ratio, a/W = 0, 0.1, 0.2, 0.3 and 0.4 for out-of-plane bending moment “i.e. loading angle φ = 0°”. For each out-of-plane bending moment and all closing and opening load angles the limit load is obtained by the tangent intersection method (TI) from the load deflection curves produced by the specially designed and constructed testing machine at the laboratory. For each out-of-plane bending moment case, the experimental results reveals that increasing crack depth leads to a decrease in the stiffness and limit load of MPB. In case of combined load (out-of-plane and in-plane opening; mode) higher load angles lead to an increase in the limit load. The highest limit load value appears at a loading angle equal, φ = 60°. In case of combined load (out-of-plane and in-plane closing; mode) the limit load decreases upon increasing the load angle. On the other hand, higher limit load values take place at a specific loading angle equal φ = 30°. For combined load opening case; higher values of limit load are obtained. Contrarily, lower values are obtained in the closing case.


Author(s):  
Kenji Oyamada ◽  
Shinji Konosu ◽  
Takashi Ohno

Pipe bends are common elements in piping system such as power or process piping, and local thinning are typically occurred on pipe bends due to erosion or corrosion. Therefore, it is important to establish the plastic collapse condition for pipe bends having a local thin area (LTA) under combined internal pressure and external bending moment. In this paper, a simplified plastic collapse assessment procedure in p-M (internal pressure ratio and external bending moment ratio) diagram method for pipe bends with a local thin area simultaneously subjected to internal pressure, p, and external out-of-plane bending moment, M, due to earthquake, etc., is proposed, which is derived from the reference stress. In this paper, only cases of that an LTA is located in the crown of pipe bends are considered. The plastic collapse loads derived from the p-M diagram method are compared with the results of both experiments and FEA for pipe bends of the same size with various configurations of an LTA.


Author(s):  
Shinji Konosu ◽  
Kenta Ogasawara ◽  
Kenji Oyamada

This paper develops a procedure for plastic collapse assessment of vessel (run pipe) - nozzle (branch pipe) intersections with an arbitrarily positioned local thin area (LTA) under different loading conditions, namely internal pressure, external moment on a nozzle applied along various directions with respect to the vessel main axis, and pure bending moment on a vessel. Although simplified procedures for plastic collapse assessment based on the p-M (internal pressure ratio and external bending moment ratio) diagram method have been previously proposed for straight cylindrical vessels and pipe bends with an LTA, very few studies have dealt with the determination of plastic collapse load for an LTA in the critical region of intersecting vessels subjected to internal pressure and external moment loading. This is likely due to the complexity of the stresses caused by the applied loads in the critical region, which arises from geometric discontinuities. In this paper, simple and empirical formulae for predicting conservative plastic collapse loads for an LTA in the critical region of the intersecting vessels are proposed based on the analytical results of stresses at defect-free vessel-nozzle intersections by using linear finite element analysis (FEA). Localized elastic stress retardation factors are taken into account in the evaluation by the results of a non-linear FEA. Consequently, a p-M diagram method is developed for application to vessel-nozzle intersections with an LTA.