Micro-tubular solid oxide fuel cell (SOFC) has been fabricated with NiO-YSZ hollow fiber as anode support and SrFe0.9Sb0.1O3−δ-Sm0.2Ce0.8O1.9(SFSb-SDC) composite cathode. The NiO-YSZ hollow fiber anode was prepared by the immersion-induced phase inversion technique and shows a special asymmetrical structure with long and large finger-like porous structure near the lumen side of the hollow fiber. A thin and dense electrolyte membrane (about 12μm) was deposited on the anode by a vacuum-assisted dip-coating process. The performance of the as-prepared micro-tubular SOFC was tested at 600-800°C with humidified H2 as fuel and ambient air as the oxidant. The peak power densities of 462.8, 336.6 and 201.4 mWcm-2can be obtained at 800, 700 and 600°C, respectively. The experimental results indicate that the cobalt-free SFSb was a promising cathode material and the prepared YSZ-based micro-tubular SOFC has potential applications as power sources for portable devices.

2011 ◽  
Vol 197-198 ◽  
pp. 672-676
Author(s):  
Jian Er Zhou ◽  
Xiao Zhen Zhang ◽  
Yong Qing Wang ◽  
Bin Lin ◽  
Xue Bing Hu ◽  
...  

Micro-tubular solid oxide fuel cell (SOFC) has been fabricated with NiO-YSZ hollow fiber as anode support and La0.6Sr0.4Co0.8Cu0.2O3−δ-Sm0.2Ce0.8O1.9 (LSCCu-SDC) composite cathode. The NiO-YSZ hollow fiber anode was prepared by the immersion-induced phase inversion technique and shows a special asymmetrical structure with porous sponge-like structure in the middle and finger-like structure on the inner and outer side of the hollow fiber. A thin and dense electrolyte membrane (about 12μm) was deposited on the anode by a vacuum-assisted dip-coating process. The performance of the as-prepared hollow fiber SOFC (HF-SOFC) was tested at 600-800°C with humidified H2 as fuel and ambient air as the oxidant. The peak power densities of 531.1, 362.5 and 214.6mWcm-2 can be obtained at 800, 700 and 600°C, respectively. The good performance at intermediate temperature (IT) indicates promising applications as power sources for portable devices for the prepared YSZ-based micro-tubular SOFCs with LSCCu-SDC composite cathode.


Author(s):  
Mazlinda Ab Rahman ◽  
Mohd Hafiz Dzarfan Othman ◽  
Hamzah Fansuri ◽  
Zawati Harun ◽  
Siti Munira Jamil ◽  
...  

2012 ◽  
Vol 523 ◽  
pp. 134-138 ◽  
Author(s):  
Dixiong Zhou ◽  
Shujun Peng ◽  
Yanying Wei ◽  
Zhong Li ◽  
Haihui Wang

2004 ◽  
Vol 30 (6) ◽  
pp. 1049-1053 ◽  
Author(s):  
Yonglian Zhang ◽  
Jianfeng Gao ◽  
Dingkun Peng ◽  
Meng Guangyao ◽  
Xingqin Liu

2010 ◽  
Vol 497 (1-2) ◽  
pp. 386-389 ◽  
Author(s):  
Xiaozhen Zhang ◽  
Bin Lin ◽  
Yihan Ling ◽  
Yingchao Dong ◽  
Guangyao Meng ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document