Effect of processing parameters on the mechanical properties of in situ compatibilized polybutylene terephthalate/acrylonitrile-butadiene-styrene blends

2011 ◽  
Vol 124 (4) ◽  
pp. 2753-2765 ◽  
Author(s):  
José Donato Ambrósio ◽  
Elias Hage
Author(s):  
Michal Jilich ◽  
Mattia Frascio ◽  
Massimiliano Avalle ◽  
Matteo Zoppi

The paper presents how a robotic gripper specific for grasping and handling of textiles and soft flexible layers can be miniaturized and improved by polymeric additive manufacturing-oriented re-design. Advantages of polymeric additive manufacturing are to allow a re-design of components with integrated functions, to be cost-effective equipment for small batches production and the availability of suitable materials for many applications. The drawback is that for design validation extended testing is still necessary because of lacks in standardization and that the mechanical properties are building parameters dependent. The outcomes are a lower complexity of the design overall and lower number of components. These are pursued taking advantage of the anisotropy of the additive manufacturing processed polymer and assigning appropriate shapes and linkages in the mechanisms. Set of common materials (polylactide, polyethylene terephthalate, acrylonitrile butadiene styrene) and technical (acrylonitrile styrene acrylate, polycarbonate/polybutylene terephthalate blend) are tested to obtain data for the modelling.


2021 ◽  
Vol 21 (9) ◽  
pp. 4840-4845
Author(s):  
Guixin Zhang ◽  
Yanyan Zhang ◽  
Jun Yang ◽  
Shijuan Li ◽  
Weihong Guo

The new wood-plastic nanocomposites (WPC) based on acrylonitrile-butadiene-styrene (ABS) resin was successfully blended with ABS and poplar flour (PF) through a HAAKE rheomix. The mechanical properties of nanocomposites, except for flexural modulus, were reduced after increasing the PF content. SEM photos show the reduction resulting from weak interfacial adhesion between the PF phase and ABS phase. Higher PF content leads to a low thermal stability and a high water absorption ratio. Different coupling agents (CA) were employed to improve the compatibility between PF and ABS. The results suggest that ABS-g-MAH is more effective than POE-g-MAH, EVA and SEBS. Maleic anhydride (MA) was blended in situ with PF and ABS as the reactive compatibilizer and mechanical properties of nanocomposites were improved except impact strength.


2012 ◽  
Vol 535-537 ◽  
pp. 2600-2605 ◽  
Author(s):  
Jian Bing Guo ◽  
Kai Zhou Zhang ◽  
Shu Hao Qin

The toughness of blends composed of PA6 and acrylonitrile-butadiene-styrene (ABS) compatibilized by using styrene-maleic anhydride (SMA) as a compatibilizer was measured over a wide temperature region. The addition of SMA results in a significant increase of the PA6 phase viscosity due to the in situ formation of graft polymers during the melt processing, and the significant change in viscosity ratio between the PA6 and ABS due to the formation of SMA-g-PA6 graft polymer may be prevent the coalescence of the dispersed phase. All results in this paper were consistent, and showed the good interaction between PA6 and ABS, which were proved by the morphology and mechanical properties of the blends.


RSC Advances ◽  
2015 ◽  
Vol 5 (61) ◽  
pp. 49143-49152 ◽  
Author(s):  
Ningjing Wu ◽  
Zhaoxia Xiu

Silicone-microencapsulated aluminum hypophosphite (SiAHP) improved effectively the flame retardancy and significantly enhanced the notched impact strength of ABS/SiAHP composites.


2019 ◽  
Vol 383 (1) ◽  
pp. 1800018 ◽  
Author(s):  
Natália Ferreira Braga ◽  
Fabio Roberto Passador ◽  
Eduardo Saito ◽  
Fernando Henrique Cristovan

Author(s):  
Shajahan Bin Maidin ◽  
Zulkeflee Abdullah ◽  
Ting Kung Hieng

One of the disadvantages of fused deposition modeling (FDM) is waste produced during the printing processes. This investigation focuses on using 100% recycled Acrylonitrile Butadiene Styrene (ABS) for the FDM process. The recycling begins with re-granule the waste ABS material and produces it into a new filament. The new recycled filament was used to print the test specimen. Investigation on the mechanical properties and the surface quality of the test specimen and comparison with standard ABS specimen was done. The result shows that the recycled ABS can be produced into filament with 335°C of extrusion temperature and 1.5 mm/s travel speed of the extruder conveyor. The surface roughness of recycled specimen is 6.94% higher than the standard ABS specimen. For ultimate tensile strength, there is a small difference in X and Y orientation between the standard and the recycled ABS specimen which are 22.93% and 19.98%, respectively. However, in Z orientation, it is 52.33% lower. This investigation proves that ABS can be recycled without significantly affecting its mechanical properties.