Application of spark plasma sintering for growing dense Pb(Mg1/3Nb2/3)O3–35 mol% PbTiO3 single crystal by solid-state crystal growth

2006 ◽  
Vol 17 (2-4) ◽  
pp. 509-513 ◽  
Author(s):  
Jong-Keuk Park ◽  
Ui-Jin Chung ◽  
Doh-Yeon Kim
2007 ◽  
Vol 336-338 ◽  
pp. 33-35
Author(s):  
Ke Pi Chen ◽  
Jin Song Pan ◽  
Xiao Wen Zhang

A small piece of <110> orientated relaxor-based ferroelectric Pb(Mg1/3Nb2/3)O3-PbTiO3 (PMN-PT) single crystals was embedded in Pb(Mg1/3Nb2/3)O3-Pb(Ni1/3Nb2/3)O3-PbTiO3 (PMN-PNN-PT) polycrystalline matrix to form the fully dense disk by spark plasma sintering (SPS) technique. Specimens were subsequently annealed to promote the boundary migration of the template single-crystal through a process termed as solid-state single crystal growth. It was found that the addition of excess 5 wt% PbO can promote the crystal growth, and the 2D morphology with V-shaped single crystals of PMN-PNN-PT were also observed. The possible growth mechanism was discussed.


2014 ◽  
Vol 2 (38) ◽  
pp. 15829-15835 ◽  
Author(s):  
Kriti Tyagi ◽  
Bhasker Gahtori ◽  
Sivaiah Bathula ◽  
A. K. Srivastava ◽  
A. K. Shukla ◽  
...  

Intrinsically ultra-low thermal conductivity and electrical transport in single-phase Cu2SbSe3 synthesized employing a solid state reaction and spark plasma sintering.


2006 ◽  
Vol 415 (1-2) ◽  
pp. 251-256 ◽  
Author(s):  
Satoru Furuyama ◽  
Tsutomu Iida ◽  
Shinsuke Matsui ◽  
Masayasu Akasaka ◽  
Keishi Nishio ◽  
...  

2005 ◽  
Vol 475-479 ◽  
pp. 2895-2898
Author(s):  
Hideki Oginuma ◽  
Katsuyoshi Kondoh ◽  
Takashi Yamaguchi ◽  
Eiji Yuasa

In this study, the solid-state reaction to form Mg2Si bulky materials via spark plasma sintering (SPS) process was discussed. Elemental powder mixture of Mg-33.33mol%Si was refined and consolidated as green compacts by repeated plastic working (RPW) SPS was performed to synthesize and sinter magnesium silicide at 1100K from the RPWed compact. The only peaks of Mg2Si, not Mg and Si, were detected by X-ray diffraction analysis. Mg2Si bulky intermetallic began to shrink above 800K during SPS process, and its densification significantly occurred. The density of SPSed Mg2Si bulk material is about 100% of the theoretically relative one.