Effect of Sintering Temperature on Properties of CNT/Al Composite Prepared by Capsule-Free Hot Isostatic Pressing Technique

2016 ◽  
Vol 70 (4) ◽  
pp. 947-955 ◽  
Author(s):  
Pham Van Trinh ◽  
Nguyen Van Luan ◽  
Phan Ngoc Minh ◽  
Doan Dinh Phuong
2017 ◽  
Vol 888 ◽  
pp. 42-46 ◽  
Author(s):  
Fatin Khairah Bahanurdin ◽  
Julie Juliewatty Mohamed ◽  
Zainal Arifin Ahmad

In this research, alkaline niobate known as K0.5Na0.5NbO3 (KNN) lead-free piezoelectric ceramic was synthesis by solid state reaction method which pressing at different sintering temperatures (1000 °C and 1080 °C) prepared via hot isostatic pressing (HIP)). The effect of sintering temperature on structure and dielectric properties was studied. The optimum sintering temperature (at 1080 °C for 30 minutes) using hot isostatic pressing (HIP) was successfully increase the density, enlarge the particle grain size in the range of 0.3 µm – 2.5 µm and improves the dielectric properties of K0.5Na0.5NbO3 ceramics. The larger grain size and higher density ceramics body will contribute the good dielectric properties. At room temperature, the excellent relative permittivity and tangent loss recorded at 1 MHz (ɛr = 5517.35 and tan δ = 0.954), respectively for KNN1080HIP sample. The KNN1080HIP sample is also exhibits highest relative density which is 4.485 g/cm3. The ɛr depends upon density and in this work, the density increase as the sintering temperature increase, which resulting the corresponding ɛr value also increases.


Sign in / Sign up

Export Citation Format

Share Document