Annealing temperature dependent oxygen vacancy behavior in SnO2 thin films fabricated by pulsed laser deposition

2011 ◽  
Vol 11 (3) ◽  
pp. S306-S309 ◽  
Author(s):  
C. Ke ◽  
W. Zhu ◽  
J.S. Pan ◽  
Z. Yang
2016 ◽  
Vol 120 (20) ◽  
pp. 205703 ◽  
Author(s):  
Abdurashid Mavlonov ◽  
Steffen Richter ◽  
Holger von Wenckstern ◽  
Rüdiger Schmidt-Grund ◽  
Michael Lorenz ◽  
...  

2009 ◽  
Vol 67 ◽  
pp. 65-70 ◽  
Author(s):  
Gaurav Shukla ◽  
Alika K. Khare

TiO2 is a widely studied material for many important applications in areas such as environmental purification, photocatalyst, gas sensors, cancer therapy and high effect solar cell. However, investigations demonstrated that the properties and applications of titanium oxide films depend upon the nature of the crystalline phases present in the films, i.e. anatase and rutile phases. We report on the pulsed laser deposition of high quality TiO2 thin films. Pulsed Laser deposition of TiO2 thin films were performed in different ambient viz. oxygen, argon and vacuum, using a second harmonic of Nd:YAG laser of 6 ns pulse width. These deposited films of TiO2 were further annealed for 5hrs in air at different temperatures. TiO2 thin films were characterized using x-ray diffraction, SEM, photoluminescence, transmittance and reflectance. We observed effect of annealing over structural, morphological and optical properties of TiO2 thin films. The anatase phase of as-deposited TiO2 thin films is found to change into rutile phase with increased annealing temperature. Increase in crystalline behaviour of thin films with post-annealing temperature is also observed. Surface morphology of TiO2 thin films is dependent upon ambient pressure and post- annealing temperature. TiO2 thin films are found to be optically transparent with very low reflectivity hence will be suitable for antireflection coating applications.


2007 ◽  
Vol 21 (10) ◽  
pp. 1775-1785 ◽  
Author(s):  
XIAN-QI WEI ◽  
BAO-YUAN MAN ◽  
YU-TAI WANG ◽  
HUI-ZHAO ZHUANG

Zinc oxide (ZnO) thin films grown on Si (111) substrates by pulsed laser deposition at O 2 ambient pressure of 1.3 Pa at different deposition temperatures have been studied. ZnO thin films underwent annealing treatment after deposition. The structural and optoelectronic properties of deposited and annealed thin films have been characterized by X-ray diffraction (XRD), atomic force microscopy (AFM), infrared absorption (IR) spectra, four-probe measurements and photoluminescence (PL) spectra. The XRD observation shows that the best crystalline quality of ZnO thin films with hexagonal structure are those grown at a temperature of 400°C and annealed at a temperature of 600°C, respectively. AFM results show that the surface roughness of the ZnO films can be decreased with increasing annealing temperature up to 600°C and then increased by further increasing the annealing temperature. The intense absorption peak sited at 417.54 cm-1 has been observed by IR spectra for ZnO film grown at 400°C and annealed at 600°C, and the property of absorption is improved by post-annealing. ZnO film grown at 400°C with a resistivity of 12.3 Ω· cm shows the best n-type semiconductor property. The PL spectra show the dominant increase in UV emission by annealing. It is concluded that the best post-annealing temperature is about 600°C.