Construction of interconnected Al2O3 doped rGO network in natural rubber nanocomposites to achieve significant thermal conductivity and mechanical strength enhancement

2020 ◽  
Vol 186 ◽  
pp. 107930 ◽  
Author(s):  
Jingchao Li ◽  
Xiuying Zhao ◽  
Zhaoxu Zhang ◽  
Yue Xian ◽  
Yutao Lin ◽  
...  
2019 ◽  
Vol 27 (4) ◽  
pp. 928-934 ◽  
Author(s):  
Junping Song ◽  
Xiteng Li ◽  
Kaiyan Tian ◽  
Lianxiang Ma ◽  
Wei Li ◽  
...  

2011 ◽  
Vol 278 ◽  
pp. 312-320 ◽  
Author(s):  
Marcos Valério Ribeiro ◽  
André Luís Habib Bahia

Considering the constant technological developments in the aeronautical, space, automotive, shipbuilding, nuclear and petrochemical fields, among others, the use of materials with high strength mechanical capabilities at high temperatures has been increasingly used. Among the materials that meet the mechanical strength and corrosion properties at temperatures around 815 °C one can find the nickel base alloy Pyromet® 31V (SAE HEV8). This alloy is commonly applied in the manufacturing of high power diesel engines exhaust valves where it is required high resistance to sulphide, corrosion and good resistance to creep. However, due to its high mechanical strength and low thermal conductivity its machinability is made difficult, creating major challenges in the analysis of the best combinations among machining parameters and cutting tools to be used. Its low thermal conductivity results in a concentration of heat at high temperatures in the interfaces of workpiece-tool and tool-chip, consequently accelerating the tools wearing and increasing production costs. This work aimed to study the machinability, using the carbide coated and uncoated tools, of the hot-rolled Pyromet® 31V alloy with hardness between 41.5 and 42.5 HRC. The nickel base alloy used consists essentially of the following components: 56.5% Ni, 22.5% Cr, 2,2% Ti, 0,04% C, 1,2% Al, 0.85% Nb and the rest of iron. Through the turning of this alloy we able to analyze the working mechanisms of wear on tools and evaluate the roughness provided on the cutting parameters used. The tests were performed on a CNC lathe machine using the coated carbide tool TNMG 160408-23 Class 1005 (ISO S15) and uncoated tools TNMG 160408-23 Class H13A (ISO S15). Cutting fluid was used so abundantly and cutting speeds were fixed in 75 and 90 m/min. to feed rates that ranged from 0.12, 0.15, 0.18 and 0.21 mm/rev. and cutting depth of 0.8mm. The results of the comparison between uncoated tools and coated ones presented a machined length of just 30% to the first in relation to the performance of the second. The coated tools has obtained its best result for both 75 and 90 m/min. with feed rate of 0.15 mm/rev. unlike the uncoated tool which obtained its better results to 0.12 mm/rev.


2012 ◽  
Vol 18 (3) ◽  
pp. 184-191 ◽  
Author(s):  
Natita Hamaviriyapornwattana ◽  
Narongrit Sombatsompop ◽  
Teerasak Markpin ◽  
Apisit Kositchaiyong ◽  
Ekachai Wimolmala

2018 ◽  
Vol 136 (13) ◽  
pp. 47281 ◽  
Author(s):  
Apinya Krainoi ◽  
Claudia Kummerlöwe ◽  
Norbert Vennemann ◽  
Yeampon Nakaramontri ◽  
Skulrat Pichaiyut ◽  
...  

2018 ◽  
Vol 936 ◽  
pp. 31-36 ◽  
Author(s):  
Wichudaporn Seangyen ◽  
Paweena Prapainainar ◽  
Pongdhorn Sae-Oui ◽  
Surapich Loykulnant ◽  
Peerapan Dittanet

Silica nanoparticles were synthesized by rice husk ash (RHA) produced from jasmine rice husk and riceberry rice husk via sol-gel method for the use as reinforcing fillers in natural rubber (NR). The obtained silica nanoparticles are spherical in shape and the particle sizes were observed to be in the 10-20 nm range with uniformly size distribution. The surface of silica nanoparticles was treated with a silane coupling agent confirmed by FTIR. The treated silica nanoparticles were then incorporated into NR and vulcanized with electron beam irradiation. The rubber nanocomposites with silica nanoparticles, produced from jasmine rice husk and riceberry rice husk, resulted in higher mechanical properties (tensile strength and modulus) than neat rubber vulcanizate. The modified rubber vulcanizates revealed rougher surface with tear lines as compared to the neat rubber vulcanizates, indicating the improved strength. Interestingly, the rubber nanocomposites with silica nanoparticles from jasmine rice husk showed higher tensile strength and modulus than silica nanoparticles produced from riceberry rice husk. The micrographs indicated better dispersion of NR composites with jasmine rice husk which leads to a strong interaction between silica nanoparticles and rubber matrix, thereby improving the strength.


1999 ◽  
Vol 35 (9) ◽  
pp. 1687-1693 ◽  
Author(s):  
N.S. Saxena ◽  
P. Pradeep ◽  
G. Mathew ◽  
S. Thomas ◽  
M. Gustafsson ◽  
...  