Magnetic separation studies for a low grade siliceous iron ore sample

2013 ◽  
Vol 23 (1) ◽  
pp. 1-5 ◽  
Author(s):  
Ranjan Kumar Dwari ◽  
Danda Srinivas Rao ◽  
Palli Sita Ram Reddy
2015 ◽  
Vol 1094 ◽  
pp. 397-400
Author(s):  
Xian Xie ◽  
Zi Xuan Yang ◽  
Xiong Tong ◽  
Ji Yong Li

Iron ore minerals are mainly silicate-type iron minerals in raw ore, and its distribution rate was 51.93%; followed by magnetic iron, and its distribution rate was 36.81%; content and distribution rate of other minerals was very low; element grade of iron, phosphorus, sulfur, silica were 11.90%, 0.043%, 0.013% and 45.23%, the main gangue were silica and calcium oxide, recyclable iron minerals mainly is magnetic iron mineral. Due to the grade of iron of raw ore and the amounts of optional magnetite was relatively little, in order to investigate the optional of low-grade ore, weak magnetic separation test and weak magnetic separation tailings-strong magnetic separation test were put into effect.


2012 ◽  
Vol 47 (8) ◽  
pp. 1129-1138 ◽  
Author(s):  
S. I. Angadi ◽  
Ho-Seok Jeon ◽  
A. Mohanthy ◽  
S. Prakash ◽  
B. Das

2014 ◽  
Vol 49 (12) ◽  
pp. 1927-1936 ◽  
Author(s):  
S. S. Rath ◽  
H. Sahoo ◽  
N. Dhawan ◽  
D. S. Rao ◽  
B. Das ◽  
...  

2012 ◽  
Vol 549 ◽  
pp. 998-1001
Author(s):  
Si Qing Liu ◽  
Peng Li ◽  
Shu Ming Wen ◽  
Dian Wen Liu

Large amount of sourrounding rocks in Jianshui China has been discarded for many years, and the “rock” is characterized by Cu-Fe polymetallic constituents and of low grade. According to the results of chemical and phase analysis as well as the mineralogy, a joint pocess of flotation and magnetic separation was proposed and used to process the ore. Flotation results show that the combined processing technology is efficient in utilizing the low grade rocks. A copper concentrate assaying 20.68% Cu at the recovery of 80.11% can be obtained, when the raw material assays 0.79% Cu.


2020 ◽  
Vol 56 (1) ◽  
pp. 47-58
Author(s):  
A. Messai ◽  
A. Idres ◽  
J.M. Menendez-Aguado

The recent developments of steel and iron industries generated a huge consumption of iron ores which has attracted much attention for utilizing low-grade iron resources to satisfy this increasing demand. The present study focuses on the characterization and enrichment of the low-grade iron ores from Rouina deposit-Ain Defla-. Currently, the ore is used in the cement industry because it is considered a low-grade iron ore. After the sampling process, a physico-chemical and mineralogical characterization was carried out and the results revealed that the sample consists of hematite, limonite and goethite as major opaque oxide minerals whereas silicates as well as clays form the gangue minerals in the sample. The average grade of FeTotal, SiO2 and Al2O3 contents in the raw material collected from the mine of the case study are 30.85%, 23.12% and 7.77% respectively. Processes involving combination of classification, washing and dry high-intensity magnetic separation were carried out to upgrade the low-grade iron ore sample to make it suitable as a marketable product. The sample was first ground and each closed size sieve fractions were subjected to washing followed by drying than dry high intensity magnetic separation and it was observed that limited upgradation is possible. As a result, it was possible to obtain a magnetic concentrate of 54.09% with a recovery degree of 89.30% and yield of 62.82% using a magnetic field intensity equal to 2.4 Tesla at the size fraction [-0.125 +0.063 mm].


2013 ◽  
Vol 641-642 ◽  
pp. 377-380
Author(s):  
Yi Miao Nie ◽  
Qi Hui Dai ◽  
Xiao Long Lu

Iron ore and tin mineral are the mainly recovered minerals of the low-grade ore, which could be effectively separated by a strong magnetic separation-gravity concentration process, with ore iron grade of 20.3%, tin grade 0.18%. Stage grinding and stage separation was used, getting the grade of iron concentrate and the recovery rate of tin separation index, the feeder of tin was magnetic separation tailing, by shaking table re-election, obtained tin concentrate grade was 10%, production was 0.34% (compared to the original ore, tin dressing) .Tin concentration ratio reached more than 330.


2013 ◽  
Vol 634-638 ◽  
pp. 3273-3276
Author(s):  
Si Qing Liu ◽  
Min Zhang ◽  
Wan Ping Wang ◽  
Xiu Juan Li

In this research, a refractory iron ore is processed, according to the basic facts of mineralogical study. Mineralogy shows that the ore is characterized by the finely disseminated iron minerals with a small amount in the ore. Iron minerals in the ore are mainly hematite and magnetite. On the basis of the ore characteristic, a flowsheet of "stage grinding-low intensity magnetic separation-high intensity magnetic separation-gravity concentration by fine shaking table" was developed. An iron concentrate assaying 51.45% Fe at a recovery of 62.12% was obtained when the raw ore contains 18.61% Fe.


Sign in / Sign up

Export Citation Format

Share Document