Photocatalytic activity of titanium dioxide nanoparticle coatings applied on autoclaved aerated concrete: Effect of weathering on coating physical characteristics and gaseous toluene removal

2012 ◽  
Vol 211-212 ◽  
pp. 218-225 ◽  
Author(s):  
Anibal Maury-Ramirez ◽  
Kristof Demeestere ◽  
Nele De Belie
2013 ◽  
Vol 331 ◽  
pp. 461-464
Author(s):  
Sheng Hui Yan ◽  
Yu Ting Zhang

t has been found that the photocatalytic activity of TiOB2B toward the decomposition of gaseous benzene in a batch reactor can be greatly improved by modifying TiOB2 Bin the presence of 3-(trimethoxysilyl) propylmethacrylate (MPS). The prepared photocatalyst (PMMA-TiOB2B) was characterized by FTIR, UV/Vis diffuse reflectance spectroscopy and XPS. PMMA-TiOB2 Bdemonstrates 2.3 times the photocatalytic activity of that of TiOB2B.


Author(s):  
Aníbal Maury Ramirez ◽  
Nele De Belie

AbstractUnder certain environmental conditions, autoclaved aerated concrete has evidenced serious problems due to the easy growth of micro-organisms such as algae. In order to prevent this situation, traditional preventive practices such as water repellents and biocide agents have been studied. Nevertheless, these efforts have not led to a complete elimination of the problem. Based on the evidence that TiO


2017 ◽  
Vol 17 (2) ◽  
pp. 284 ◽  
Author(s):  
Leny Yuliati ◽  
Nur Azmina Roslan ◽  
Wai Ruu Siah ◽  
Hendrik Oktendy Lintang

2,4-dichlorophenoxyacetic acid (2,4-D) has been recognized as a possibly carcinogenic compound to human, therefore, 2,4-D should be treated before it is discharged to the environment. Photocatalytic degradation of 2,4-D has been proposed as one of the best methods that offer environmentally safe process. In the present research, titanium dioxide (TiO2) was modified with cobalt oxide (CoO) and tested for photocatalytic degradation of 2,4-D under UV light irradiation. Different amounts of CoO (0.1, 0.5, 1 and 5 mol%) were added onto TiO2 by an impregnation method. The photocatalytic reaction was monitored and analyzed by measurement of 2,4-D absorbance using UV spectrophotometer. After 1 h photocatalytic reaction, it was confirmed that the sample with low loading of 0.1 mol% gave the highest photocatalytic activity among the bare and modified TiO2 photocatalysts. The photocatalytic activity was decreased with the increase of CoO loading, suggesting that the optimum amount of CoO was an important factor to improve the performance of TiO2. Based on fluorescence spectroscopy, such addition of CoO resulted in the reduced emission intensity, which showed the successful decrease in the electron-hole recombination.


2012 ◽  
Vol 2012 ◽  
pp. 1-10 ◽  
Author(s):  
Siti Hajar Othman ◽  
Suraya Abdul Rashid ◽  
Tinia Idaty Mohd Ghazi ◽  
Norhafizah Abdullah

To produce titanium dioxide (TiO2) nanoparticle coatings, it is desirable that the nanoparticles are dispersed into a liquid solution and remain stable for a certain period of time. Controlling the dispersion and aggregation of the nanoparticles is crucial to exploit the advantages of the nanometer-sized TiO2particles. In this work, TiO2nanoparticles were dispersed and stabilized in aqueous suspensions using two common dispersants which were polyacrylic acid (PAA) and ammonium polymethacrylate (Darvan C). The effect of parameters such as ultrasonication amplitude and type and amount of dispersants on the dispersibility and stability of the TiO2aqueous suspensions were examined. Rupture followed by erosion was determined to be the main break up mechanisms when ultrasonication was employed. The addition of dispersant was found to produce more dispersed and more stabilized aqueous suspension. 3 wt.% of PAA with average molecular weight (Mw) of 2000 g/mol (PAA 2000) was determined to produce the best and most stable dispersion. The suspensions were then coated on quartz glass, whereby the photocatalytic activity of the coatings was studied via the degradation of formaldehyde gas under UV light. The coatings were demonstrated to be photocatalytically active.