Rapid synthesis of dense NiTi alloy through spark plasma sintering of a TiH2/Ni powder mixture

2017 ◽  
Vol 191 ◽  
pp. 89-92 ◽  
Author(s):  
Bolu Liu ◽  
Shuigen Huang ◽  
Liugang Chen ◽  
Jan Van Humbeeck ◽  
Jef Vleugels
2021 ◽  
Vol 11 (4) ◽  
pp. 1802
Author(s):  
Sneha Samal ◽  
Orsolya Molnárová ◽  
Filip Průša ◽  
Jaromír Kopeček ◽  
Luděk Heller ◽  
...  

An analysis of the shape memory effect of a NiTi alloy by using the spark plasma sintering approach has been carried out. Spark plasma sintering of Ti50Ni50 powder (20–63 µm) at a temperature of 900 °C produced specimens showing good shape memory effects. However, the sample showed 2.5% porosity due to a load of 48 MPa. Furthermore, an apparent shape memory effect was recorded and the specimens were characterized by uniformity in chemical composition and shape memory alloys of NiTi showed significant austenite phases with a bending strain recovery of >2.5%.


2014 ◽  
Vol 122 (1425) ◽  
pp. 336-340 ◽  
Author(s):  
Ievgen SOLODKYI ◽  
Hanna BORODIANSKA ◽  
Ting ZHAO ◽  
Yoshio SAKKA ◽  
Petre BADICA ◽  
...  

2018 ◽  
Vol 120 ◽  
pp. 218-222 ◽  
Author(s):  
Weibing Zhou ◽  
Kang Li ◽  
Jiaoqun Zhu ◽  
Shouqin Tian

2014 ◽  
Vol 1040 ◽  
pp. 772-777 ◽  
Author(s):  
Lilia I. Shevtsova ◽  
Michail A. Korchagin ◽  
Alexander Thömmes ◽  
Vyacheslav I. Mali ◽  
Alexander G. Anisimov ◽  
...  

In this paper structure and mechanical properties of Ni3Al intermetallic compound was studied. The materials was fabricated according to different schemes, which combined mechanical alloying of Ni and Al powders, self-propagating high temperature synthesis (SHS) and spark plasma sintering (SPS). Relative density of all sintered samples was ~ 97 %. Microhardness of the sintered materials ranged from 6100 to 6300 MPa. SPS of 86.71 % wt. Ni and 13.29 % wt. Ni powder at 1100 °C led to formation of material with the highest level of tensile strength equal to 400 MPa.