Improvement in corrosion resistance of the 316l stainless steel by means of Al2O3 coatings deposited by the sol-gel method

1999 ◽  
Vol 349 (1-2) ◽  
pp. 186-190 ◽  
Author(s):  
J Masalski ◽  
J Gluszek ◽  
J Zabrzeski ◽  
K Nitsch ◽  
P Gluszek
2012 ◽  
Vol 1449 ◽  
Author(s):  
Chen Zhao ◽  
Dan Jiang ◽  
Shundong Bu ◽  
Jinrong Cheng

ABSTRACTFerroelectric 0.7BiFeO3-0.3PbTiO3 (BFO-PT) films were deposited on stainless steel substrates by the sol-gel method. A thin layer of PbTiO3 (PT) was introduced between the substrates and BFO-PT films in order to decrease the annealing temperature of BFO-PT films. X-ray diffraction analysis reveals that BFO-PT films could be well crystallized into the perovskite structure at about 575 oC. Scanning electron microscope (SEM) images show that BFO-PT thin films have grain size of about 50∼60 nm. Our results indicated BFO-PT films deposited on stainless steel substrates maintained the excellent ferroelectric properties with remnant polarization of about 40∼50 μC/cm2.


Sign in / Sign up

Export Citation Format

Share Document