Structural and Electrochemical Study of the Li–Mn–Ni Oxide System within the Layered Single Phase Region

2014 ◽  
Vol 26 (24) ◽  
pp. 7059-7066 ◽  
Author(s):  
Jing Li ◽  
John Camardese ◽  
Stephen Glazier ◽  
J. R. Dahn
1962 ◽  
Vol 40 (10) ◽  
pp. 1397-1400 ◽  
Author(s):  
W. Klement Jr.

By rapidly cooling liquid alloys, single-phase nickel-rich solid solutions have been obtained to [Formula: see text] at.% tin, ~20 at.% germanium, and [Formula: see text] at.% silicon. The lattice parameters measured for the metastable structures as well as for some alloys within the equilibrium single-phase region suggest linear variations with solute content, with slopes (in units of 10−3 Å/at.% solute) of +8.5 for tin, +1.94 for germanium, and −0.55 for silicon.