NICKEL-RICH SOLID SOLUTIONS IN BINARY ALLOYS WITH TIN, GERMANIUM, AND SILICON

1962 ◽  
Vol 40 (10) ◽  
pp. 1397-1400 ◽  
Author(s):  
W. Klement Jr.

By rapidly cooling liquid alloys, single-phase nickel-rich solid solutions have been obtained to [Formula: see text] at.% tin, ~20 at.% germanium, and [Formula: see text] at.% silicon. The lattice parameters measured for the metastable structures as well as for some alloys within the equilibrium single-phase region suggest linear variations with solute content, with slopes (in units of 10−3 Å/at.% solute) of +8.5 for tin, +1.94 for germanium, and −0.55 for silicon.


1963 ◽  
Vol 41 (5) ◽  
pp. 758-761 ◽  
Author(s):  
Huey-Lin Luo ◽  
Pol Duwez

By rapidly cooling liquid alloys, single-phase face-centered cubic cobalt-rich solid solutions have been obtained with up to 17.2 at.% aluminum, 18.2 at.% gallium, 13 at.% silicon, 17.4 at.% germanium, and 5 at.% tin. With the exception of silicon, these limits of solubility exceed those found under equilibrium conditions. The variation of lattice parameter with composition has been measured and the data can be fitted with straight lines for all solute elements except gallium, in which a change of slope is observed at 13.2 at.%.



1973 ◽  
Vol 56 (1) ◽  
pp. K17-K20 ◽  
Author(s):  
Y. Aoki ◽  
T. Nakamichi ◽  
M. Yamamoto